| Cr5Mo异种钢焊接熔合区H2S腐蚀过程的原位观察 |
| 邹 杨; 潘春旭;傅 强; 陈 超 |
| 武汉大学物理科学与技术学院; 武汉 430072 |
|
| In Situ Observations For Corrosion Process At Fusion Boundary Of Cr5Mo Dissimilar Steel Welded Joints In H2S Containing Solution |
| ZOU Yang; PAN Chunxu; FU Qiang; CHEN Chao |
| Department of Physics; Wuhan University; Wuhan 430072 |
引用本文:
邹杨; 潘春旭; 傅强; 陈超 . Cr5Mo异种钢焊接熔合区H2S腐蚀过程的原位观察[J]. 金属学报, 2005, 41(4): 421-426 .
,
,
,
.
In Situ Observations For Corrosion Process At Fusion Boundary Of Cr5Mo Dissimilar Steel Welded Joints In H2S Containing Solution[J]. Acta Metall Sin, 2005, 41(4): 421-426 .
[1]Huang H H, Lee J T, Tsai W T. Mater Chem Phys, 1999; 58: 177 [2]Dong P, Zhang J. Eng Fracture Mech, 1999; 64: 485 [3]Li G F, Charles E A, Conleton J. Corros Sci, 2001; 43: 1963 [4]Guo H, Cai X, Yang W. Mater Mech Eng, 2002; 26(4): 1 (郭浩,蔡洵,杨武.机械工程材料,2002;26(4):1) [5]Liu L W, Hu Q, Guo F, Zhao X Q, Wu J J. Corros Prot, 2002; 23(1): 10 (刘烈炜,胡倩,郭枫,赵新强,吴建军.腐蚀与防护,2002; 23(1):10) [6]Zhang X C, Gong J M, Tu S D, Ling X. Pet Refinery Eng, 2003; 33(10): 25 (张显程,巩建鸣,涂善东,凌 详.炼油技术与工程, 2003; 33(10):25) [7]Li Y T, Du Z Y, Tao Y Y, Xiong L Y. Trans Chin Weld Inst, 2003; 24(3): 76 (李云涛,杜则裕,陶勇寅,熊林玉.焊接学报, 2003;24(3): 76) [8]Pan C X. Dissimilar Steel and Dissimilar Metal Welding Micro structural Characterization and Transformation Behavior. Beijing: People's Communication Press, 2000: 36 (潘春旭.异种金属焊接-显微结构特征及其转变机理.北京: 人民交通出版社,2000:361 [9]Lundin C D. Weld J, 1982; 61(2): 58-s [10]Faber G, Gooch T G. Welding World, 1982; 20(5/6): 87 [11]Li Z Y. Corros Prot, 1977; 14(1): 51 (李祖贻.石油化工腐蚀与防护, 1997;14(1):51) [12]NACE Standard TM 0177, National Association of Corrosion Engineers, Houston, TX, 1990 [13]Xu J, Zhong M Y, Guo S X, Hardie D. J Chin Soc Corros Prot, 2003; 23(3): 149 (徐坚,钟曼英,郭士行,Hardie D.中国腐蚀与防护学报, 2003;23(3):149) [14]Yu G, Zhang X Y, Ke K. Petrochem Corros Prot, 1999; 16(4): 51 (余刚,张学元,柯克.石油化工腐蚀与防护,1999;16(4): 51) [15]Morishige N, Kume R, Okabayashi H. Trans Jpn Weld Soc, 1985; 16(1): 12 [16]Kinoshita K, Ito H, Ebata A, Hattori T. Trans ISIJ, 1985; 25: 505 [17]Brouwer R C. Int J Pres Ves Piping, 1993; 56: 133 [18]Pan C, Zhang Z. Mater Charact, 1994; 33(2): 87 [19]Li Y S, Niu Y, Wu W T. Corros Sci Prot Technol, 2000; 12: 41 (李远士,牛焱,吴维(?).腐蚀科学与防护技术, 2000;12: 41) [20]Liu P. PhD Dissertation, Knoxville, USA: The University of Tennessee, 2001 [21]Pan C, Li A, Sun G, Holmquist M. Mater Sci Technol, 1998; 14(3): 201L |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|