| GMAW焊接熔滴过渡动态过程的数值分析 |
| 陈茂爱; 武传松; 廉 荣 |
| (山东大学材料液态结构及其遗传性教育部重点试验室; 济南 250061) |
|
引用本文:
陈茂爱; 武传松; 廉荣 . GMAW焊接熔滴过渡动态过程的数值分析[J]. 金属学报, 2004, 40(11): 1227-1232 .
[1] Amson J C. Brit Weld J, 1962; 41(4) : 232 [2] Kim Y S, Eagar T W. Weld J, 1993; 72(6) : 269s [3] Allum C J. J Phys D: Appl Phys, 1985; 18(6) : 1431 [4] Allum C J. J Phys D: Appl Phys, 1985; 18(6) : 1447 [5] Haidar J, Lowke J. J Phys D: Appl Phys, 1996; 29(6) :2951 [6] Choi S K, Yoo C D, Kim Y S. Weld J, 1998; 77(1) : 28s [7] Fan H G, Kovacevic R. Metall Mater Trans, 1999; 30B(8) :791 [8] Fan H G, Kovacevic R. J Phys D: Appl Phys, 1998; 31:2929 [9] Hirt C W, Nichols B D. J Comp Phys, 1981; 39(2) : 201 [10] Lancaster J F. The Physics of Welding. New York: Perg-amon, 1986U |
|