| 电弧离子镀沉积Al(Cr)--O--N扩散阻挡层的研究 |
| 王启民;武颖娜;纪爱玲 |
| 中国科学院金属研究所金属腐蚀与防护国家重点实验室 |
|
| Study Of Al--O--N And Cr--O--N Films Deposited By Arc Ion Plating As Diffusion Barriers |
| WANG Qimin; WU Yingna; JI Ailing |
| State Key Laboratory for Corrosion and Protection;Institute of Metal Research;The Chinese Academy of Sciences |
引用本文:
王启民; 武颖娜; 纪爱玲 . 电弧离子镀沉积Al(Cr)--O--N扩散阻挡层的研究[J]. 金属学报, 2004, 40(1): 83-87 .
,
,
.
Study Of Al--O--N And Cr--O--N Films Deposited By Arc Ion Plating As Diffusion Barriers[J]. Acta Metall Sin, 2004, 40(1): 83-87 .
[1] Rhys-Jones T N. Corros Sci, 1989; 29:623 [2] Morral J E, Thompson M S. Surf Coat Technol, 1990; 43/44:371 [3] Coad J P, Rickerby D S. Mat Sci Eng, 1985; 74:93 [4] Lou H Y, Wang F H. Vacuum, 1992; 43:757 [5] Knotek O, Loffler F, Beele W. Surf Coat Technol, 1993;61:6 [6] Knotek O, Lugscheider E, L6ffier F, Beeler W. Surf Coat Technol, 1994; 68/69:26 [7] Cremer R, Witthaut M, Reichert K, Schierling M, Neuschütz D. Surf Coat Technol, 1998; 108/109:48 [8] Reichert K. Surf Eng, 1999; 15(2) : 163 [9] Müller J, Schierling M, Zimmermann E, Neuschütz D. Surf Coat Technol, 1999; 120/121:16 [10] Richthofen A V, Domnick R. Thin Solid Films, 1996; 283:37 [11] Liang Y J, Che Y C. Handbook of Thermodynamic Data for Inorganic Compounds. Shenyang: Northeast University Press, 1993: 49, 51, 122, 123(梁英教,车萌昌.无机物热力学数据手册.沈阳:东北大学出版社,1993:49,51,122,123) [12] Li M S. High Temperature Corrosion of Metals. Beijing: Metallurgy Industry Press, 2001:43(李美栓.金属的高温腐蚀.北京:冶金工业出版社,2001:43) [13] Lou H Y. J Chin Soc Corros Protect, 1997; 17(Suppl.): 464(楼翰一.中国腐蚀与防护学报.1997;17(增刊):464) |
|