| Pd/Y薄膜在气态吸放氢过程中的表面形貌和可转换光学特性 |
| 张文魁 黄辉 甘永平 |
| 浙江工业大学化工学院; 杭州310014 |
|
引用本文:
张文魁; 黄辉; 甘永平 . Pd/Y薄膜在气态吸放氢过程中的表面形貌和可转换光学特性[J]. 金属学报, 2003, 39(9): 974-978 .
[1] Huiberts J N, Rector J H, Wijngaarden R J, Jetten S,Groot D G, Dam B, Koeman N J, Griessen R. J AlloysCompd, 1996; 239: 158 [2] Huiberts J N, Griessen R, Rector J H, Wijingaarden R J,Dekker J P, Groot D G, Loeman N J. Nature, 1996; 231:380 [3] Griessen R, Huiberts J N, Kremers M, Gogh A, KoemanN J, Dekker J P, Notten, P H L. J Alloys Compd, 1997;(253-254) : 44 [4] Sluis P. Appl Phys Lett, 1997; 70: 3356 [5] Sluis P. Appl Phys Lett, 1998; 73: 1826 [6] Nagengast D G, Gogh A, Kooij E S. Appl Phys Lett, 1999;75: 2050 [7] Gogh A, Kooij E S, Griessen R. Phys Rev Lett, 1999; 83:4614 [8] Notten P H L, Kremers M, Griessen R. J Electrochem Soc,1996; 143: 3348 [9] Matveeva T, Parkhutik V. J Electrochem Soc, 2002; 149:D148 [10] Zhang L D. Preparation and Application of SuperfinePowder. Beijing: Chinese Petrochemical Press, 2001: 239(张立德.超微粉体制备与应用技术.北京:中国石化出版社,2001:239 [11] Yang B Z, Wang W S. Physics and Technology of Thin Films. Xi'an: Xi'an University of Electron Science and Technology Press, 1994: 169(杨邦朝,王文生.薄膜物理与技术,西安:西安电子科技大学出版社, 1994:169) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|