| 新型Zr-Al-Ni-Cu块状非晶合金 |
| 刘海军 阵伟荣 王英敏 |
| 大连理工大学三束材料改性国家重点联合实验室; 大连116024 |
|
引用本文:
刘海军 ; 阵伟荣; 王英敏 . 新型Zr-Al-Ni-Cu块状非晶合金[J]. 金属学报, 2003, 39(9): 938-942 .
[1] Inoue A, Zhang T, Masumoto T. Mater Trans JIM, 1989;30: 965 [2] Inoue A, Kita K, Zhang T, Masumoto T. Non-CrystSolids, 1993; 156-158: 473 [3] Peker A L, Johnson W L. Appl Phys Lett, 1993; 63, 2342 [4] Inoue A, Zhang T. Masumoto J. Non-Cryst Solids, 1993;156-158: 473 [5] Inoue A. Mater Sci Forum, 1995; 691: 179-181 [6] Nagel S R, Tauc J. Phys Rev Lett, 1975; 35: 380 [7] Haussler P. Phys Rep, 1992; 222(2) : 65 [8] Hafner J, Krajci M. Phys Rev, 1993; B47: 11795 [9] Mizutani U, Takeuchi T. Sato Prog Mater Sci, 2003, inPress [10] Shek C H, Wang Y M, Dong C. Mater Sci Eng, 2000;A291: 78 [11] Wang Y M, Qiang J B, Wong H C, Shek C H, Dong C. JMater Res, 2003; 18: 642 [12] Chen W R, Wang Y M, Qiang J B, Dong C. Acta MetallSin, 2002; 38: 421(陈伟荣,王英敏,羌建兵,董闯.金属学报,2002;38:421) [13] Chen W R. Ph D Thesis, Dalian: Dalian University of Technol, 2002(陈伟学.大连理工大学博士论文,大连,2002) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|