| 1500 MPa级贝氏体/马氏体复相高强度钢的疲劳断裂特性 |
| 韦东远 顾家琳 方鸿生 |
| 清华大学材料科学与工程系先进材料教育部重点实验室100084 |
|
引用本文:
韦东远; 顾家琳; 方鸿生 . 1500 MPa级贝氏体/马氏体复相高强度钢的疲劳断裂特性[J]. 金属学报, 2003, 39(7): 734-738 .
[1] Tomita Y, Okabayashi K. Metall Trans, 1983; 14A: 485 [2] Tomita Y, Obabayashi K. Metall Trans, 1985; 16A: 73 [3] Tomita Y, Okabayashi K. Metall Trans, 1983; 14A: 2387 [4] Yu M T, Topper T H, Wang L. Int J Fatigue, 1988; 10: 249 [5] Fang H S, Zheng Y K, Chen X Y, Zhao R, Zhou X. J Met, 1988; 40(3) : 51 [6] Huang W G, Fang H S, Zheng Y K. Trans Met Heat Treat, 1997; 18(1) : 8(黄维刚,方鸿生,郑燕康.金属热处理学报,1997;18(1) :8) [7] Fang H S, Liu D Y, Xu P G, Bai B Z, Yang Z G. Mater Mech Eng, 2001; 25(6) : 1(方鸿生,刘东雨,徐平光,白秉哲,杨志刚.机械工程材料,2001;25(6) :1) [8] Moore T D. Structural Alloys Handbook. Vol.1, Traverse City, Michigan: Mechanical Properties Data Center, Belfour Stulen, Inc., 1975: 97 [9] Berns H, Wener L. Theor Appl Fract Mech, 1986; 6: 11 [10] Miihkinen V T T, Edmonds D V. Mater Sci Technol, 1987; 6: 441 [11] Ritchie R O, Castrocedeno M H, Zackay V F, Parker E R Metall Trans, 1978; 9A: 35 [12] Fleck N A. In: Smith R A, ed., Fatigue Crack Growth 30 Years of Progress, Oxford: Pergamon Press, 1986: 75 [13] Beevers C J, Carlson R L. In: Smith R A, ed., Fatigue Crack Growth 30 Years of Progress, Oxford: Pergamon Press, 1986: 89 [14] Elber W. Eng Fract Mech, 1970; 2: 37 [15] Paris P C, Bucci R J, Wessel E T, Clarke W G, Mager T R. ASTM STP 513, 1972 [16] Stewart A T. Eng Fract Mech, 1980; 13: 463 [17] Suresh S, Ritchie R O. Metall Trans, 1982; 13A: 1627 [18] Halliday M D, Beevers C J. Int J Fract, 1979; 15(1) : R27 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|