| 超极钢焊接接头粗晶区的精细结构 |
| 赵玉珍 李擘 史耀武 |
| 北京工业大学材料科学与工程学院100022 |
|
引用本文:
赵玉珍; 李擘; 史耀武 . 超极钢焊接接头粗晶区的精细结构[J]. 金属学报, 2003, 39(5): 505-509 .
[1] Sato A. Proc Int Conf Ultra Steel 2000, Tsukuba, Japan, 2000: 1 [2] Niikura M, Fujioka M, Adachi Y, Matsakara A, Yokota T. J Mater Process, 2001; 117: 341 [3] Worr P L. Development of High Performance Structural Steels for 21st Century in Korea. Tsukuba, Japan, 2000: 179 [4] Peng Y, Wang C, Chen W Z, Tian Z L. Trans Chin Weld Inst, 2002; 22: 32(彭云,王成,陈武柱,田志凌.焊接学报,2002;22:32) [5] Tian Z L, He C H, Zhang X M, Zou G, Qu Z X. Trans Chin Weld Inst, 2001; 22: 1(田志凌,何长红,张晓牧,邹钢,屈朝霞 焊接学报,2001;22:1) [6] Tian Z L. The Conference Document of Metal Weldability and Welding Materials Committee, Beijing, 2000(田志凌.金属焊接性与焊接材料委员会会议论文,北京,2000) [7] Qu Z X, Tian Z L, He C H, Zhang X M, Yang B, Cao N. Iron Steel, 2000; 35: 70(屈朝霞,田志凌,何长红,张晓牧,杨柏,曹能.钢铁,2100;35:70) [8] Qu Z X. Ph D Thesis, Tianjin University, Tianjin, 2000(屈朝霞.天津大学博士学位论文,天津,2000) [9] Kang M K, Yang S P, Guan D H. Bainites in Steels. Shanghai: Shanghai Science and Technology Press, 1990: 175(康沫狂,杨思品,管敦惠.钢中贝氏体.上海:上海科学技术出版社,1990:175 [10] Quidort D, Bre‘chet Y. Scr Mater, 2002; 47: 151 [11] Fang H S, Yang J B, Yang Z G, Bai B Z. Scr Mater, 2002; 47: 157 [12] Van S, Wang J. Scr Mater, 2002; 47: 163 [13] Hehemann R F. Phase Transformation. Metals Park, Ohio: ASM, 1968: 397 [14] Yu D G. The Theory of Bainite Transformation. Shanghai: Shanghai Jiaotong University Press,1992: 22(俞德刚.贝氏体相变理论.上海:上海交通大学出版社,1998:22) [15] Li F Z, Ao Q, Gu Y N, Jiang J, Sun D S. Acta Metall Sin, 1997; 33: 241(李凤照,敖青,顾英妮,姜江,孙东升.金属学报,1997;33:241)a |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|