| Cr-Mn-N奥氏体-铁素体不锈钢的空蚀行为 |
| 柳伟;郑玉贵;刘常升;姚治铭;柯伟 |
| 中国科学院金属研究所金属腐蚀与防护国家重点实验室;沈阳 110016;东北大学材料与冶金学院;沈阳 110004 |
|
| Cavitation Erosion Behavior of Cr-Mn-N Austenite-Ferrite Stainless Steel |
| LIU Wei; ZHENG Yugui; LIU Changsheng; YAO Zhiming; KE Wei |
| State Key Laboratory for Corrosion and Protection; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016; School of Materials & Metallurgy; Northeastern University; Shenyang 110004 |
引用本文:
柳伟; 郑玉贵; 刘常升; 姚治铭; 柯伟 . Cr-Mn-N奥氏体-铁素体不锈钢的空蚀行为[J]. 金属学报, 2003, 39(1): 85-88 .
,
,
,
,
.
Cavitation Erosion Behavior of Cr-Mn-N Austenite-Ferrite Stainless Steel[J]. Acta Metall Sin, 2003, 39(1): 85-88 .
[1] Fu W T, Jing T F, Zheng Y Z, Yao M, He X K. J Iron Steel Res, 1997; 9: 38(傅万堂,荆天辅,郑炀曾,姚枚,何筱奎.钢铁研究学报,1997;9:38) [2] Institute of Metal Research, The Chinese Academy of Sciences. Fushun Special Steel Factory. Research on Cr-Mn-N Non-Nickel Stainless Steels. Beijing: Science Press, 1969: 1(中国科学院金属研究所,抚顺特殊钢厂.铬锰氮无镍不锈钢的研究.北京:科学出版社, 1969:1) [3] Kwok C T, Man H C, Leung L K. Wear, 1997, 211: 84 [4] Kwok C T, Man H C, Cheng F T. Maer Sci Eng, 1998;A242: 108 [5] Wang Z C, Zhang X Q. In: Gu S H ed, Abrasion andCavitation in Hydraulic Machinery, Tianjin, 1999-2000;68(王者昌,张晓强.见:顾四行编,水机磨蚀,天津,1999-2000;68) [6] Fu W T, Jing T F, Zheng Y Z, Yao M. J Mater EngPerfor, 1998; 7: 801 [7] Liu W, Zheng Y G, Yao Z M, Ke W. Chin J Mater Res,2001; 15: 505(柳伟,郑玉贵,姚治铭,柯伟.材料研究学报,2001;15:505) [8] Gonalez J L, Aranda R, Jonapa M. Application of Stainless Steel' 92, Stockholm, Sweden, 1992; 2: 1009 [9] Al-Hashem A, Caceres P G, Bdullah A A, Shalaby H M.Corrosion, 1997; 53(2) : 103 [10] Shalaby H M. Corrosion'96, Denver: Colorado, 1996: 497 [11] Preece C M. Cavitation Erosion, In: Preece CM ed, Treatise on Material Science and Technology, New York: Academic Press, 1979; 16: 249 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|