CrMnB堆焊合金抗空蚀和冲刷磨损性能的研究 |
国旭明 郑玉贵 姚治铭 |
中国科学院金属研究所金属腐蚀与防护国家重点实验室;沈阳110016 |
|
引用本文:
国旭明; 郑玉贵; 姚治铭 . CrMnB堆焊合金抗空蚀和冲刷磨损性能的研究[J]. 金属学报, 2002, 38(9): 936-940 .
[1] Gu S H. Large Electricity Machinery Technique, 1982; (3): 48(顾四行.大电机技术,1982;(3):48) [2] Wang Z C, Zheng F Z, Bai L M. In: Gu S H ed. Abrasion and Cavitation in Hydraulic Machinery. Tianjin: Yellow River Hydro-Power Press, 1993: 151 (王者昌,郑风珍,白良谋.见:顾四行编.水机磨蚀.天津: 黄河水利出版社,1993:151) [3] Heathcock C J, Protheroe B E, Ball A. Wear, 1982; 81:311 [4] Kwok C T, Man H C, Cheng F T. Surf Coat Technol,2000; 126: 238 [5] Fu W T, Zhang D S. Iron Steel, 1999; 34 : 42 (傅万堂,张东升.钢铁,1999;34:42) [6] Iwai Y, Okada T, Awazu K, Hammitt F G. Wear, 1982;79: 283 [7] Schramm R E. Metall Trans, 1975; 6A: 1345 [8] Li J M. Wear Metallography. Beijing: Metallurgy Indus-try Press, 1990: 233 (李建明.磨损金属学.北京:冶金工业出版社,1990:233) [9] Zhao K, Gu C, Shen F, Lou B. Wear, 1993; 162-164: 811z |
|