| Zr55Al10Ni5Cu30块状非晶合金的高温压缩断裂 |
| 张庆生 张海峰 王爱民 丁炳哲 胡壮麒 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室;沈阳110016 |
|
引用本文:
张庆生; 张海峰; 王爱民; 丁炳哲; 胡壮麒 . Zr55Al10Ni5Cu30块状非晶合金的高温压缩断裂[J]. 金属学报, 2002, 38(8): 835-838 .
[1] Zhang T, Inoue A, Masumoto T. Mater Trans JIM, 1991;32: 1005 [2] Peker A, Johnson W L. Appl Phys Lett, 1993; 63: 2342 [3] Inoue A, Zhang T, Masumoto T. Mater Trans JIM, 1991;31: 177 [4] Kim S G, Inoue A, Masumoto T. Mater Trans JIM, 1991;31: 929 [5] Leamy H J, Chen H S, Wang T T. Metall Trans, 1972; 3:699 [6] Liu C T, Heatherly L, Easton D S, Carmichael C A, Schneibel J H, Chen C H, Wright J L, Yoo M H, Hor-ton J A, Inoue A. Metall Mater Trans, 1998; 29A: 1811 [7] Bruck H A, Rosakis A J, Johnson W L. J Mater Res, 1996;11: 503 [8] Spaepen F. Ada Metall, 1977; 25: 407 [9] Argon A S. Ada Metall, 1979; 27: 47 [10] Wright W J, Saha R, Nix W D. Metall Mater Trans, 2001;42: 642 [11] Pampillo C A. J Mater Sci, 1975; 10: 1194 [12] Davis L A, Das S K, Li J C M, Zedalis M S. Int J RapiaSolidif, 1994; 8: 73 [13] Hufnagel T C, El-deiry P, Vinci R P. Scr Mater, 2000; 43:1071 [14] Inoue A. Acta Mater, 2000; 48: 279 [15] Inoue A. Bulk Amorphous Alloys. Zurich: Trans Technol. Publications, 1998: 2 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|