Please wait a minute...
金属学报  2002, Vol. 38 Issue (1): 84-90     
  论文 本期目录 | 过刊浏览 |
化学镀多元非晶态合金形成规律探讨
王玲玲 黄维清
湖南大学材料科学与工程学院;长沙410082
引用本文:

王玲玲; 黄维清 . 化学镀多元非晶态合金形成规律探讨[J]. 金属学报, 2002, 38(1): 84-90 .

全文: PDF(258 KB)  
摘要: 利用二维Miedeman坐标(△φ^*和△n^-1/3W-S)以及加入尺寸因素△RRA构成的三维化学坐标揭示了化学镀多元合金的非晶形成规律,对已有实验结果的60个化学镀多元合金系分析表明,非晶化条件为:二维坐标系中,二元和三元体系,|△φ^*|>6.9|△n^-1/3W-S|;二元,三地和四元体系,|△φ^*|>6.9|△n^-1/3W-S|+0.1,三维坐标系中,二元体系|△R/RA|>0.18[1-|△n^-1/3W-S|/(-0.01)-|△φ^*|/0.08|,二元和三元体系,|△R/RA|>0.14[1-|△n^-1/3W-S|/(-0.01)-|△φ^*|/0.O8];二元,三元和四元体系,|△R/RA|>0.26[1-|△n^-1/3W-S|/(-0.01)-|△φ^*|/0.07]。二元和三元合金系统的区分准确率高于84%,四元合金体系的区分准确率高于81%.
关键词 : 化学镀,  多元合金,  非晶形成规律,  Miedema理论    
Key words:
收稿日期: 2001-03-20     
ZTFLH:  TG139.8 TQ153.2  
[1]  Cohen H M, Turnbull D. Nature. 1961; 189:  131 
[2]  Ouyang Y F, Zhong X P, Chen H M. Acta Metall Sin. 1999; 35:  1095(欧阳义芳,钟夏平,陈红梅. 金属学报.1999; 35:1095)
[3]  Mader S, Nowick A S, Widmer H. Acta Metall, 1967; 15:203 
[4]  Benedictus R, Bottger A, Mittemeijer E J.  Z Metallkd,1998; 89:  168 
[5]   Alonso J A, Simozar S.  Solid State  Commun,  1983; 49:765 
[6]  Ning Y T, Zhou X M. Acta Metall Sin, 1981; 17: 278(宁远涛,周新铭 金属学报,1981;17:278)
[7]  Daroczi   C   S,   Dora   G.   Horvath   Z   E,   Homonnay   Z,Idzikowski B.  Vacuum, 1998; 50: 343
[8]   Brower W, Megli S. Mater Sci Eng, 1991; 133A: 846 
[9]  Leng Y, Courtney T H. J Mater Sci, 1991; 26: 588 
[10]  Goncalves A P, Almeida M. Physica, 1996; 228B: 289 
[11] Gallego L J, Somoga J A, Alonso J A. J Phys CondensMatter, 1990; 2: 6245
[12]  Xu Z Y. Metal Material Thermodynamics.   Beijing:  Science Press, 1981: 227
(徐祖耀 金属材料热力学. 北京:科学出版社、1981:227)
[13]  Zhang B W. Xie H W, Liao S Z. J Mater Process Technol, 1999: 89: 378Zhang B W, Xie H W, Liao S Z.  Trans Inst Met Finish, 1996; 74: 69Zhang B W, Xie H W, Liao S Z. Rare Met Mater Eng, 1998; 27: 79Zhang BW, Xie H W. Liao S Z.  Mater Sci Eng, 2000; 281A: 286 
[14]  Chen N Y. Zhang X G. Acta Chem, 1975; 33:  101
(陈念贻,章兴国 .化学学报、1975:33:101)
[15]  Zhang B W. Physica, 1985; 132B: 319 Zhang B W. Physica, 1983; 121B: 405 Zhang B W. Phys Status Solidi, 1987; 102A: 199 Zhang B W. J Mater Sci Lett, 1988; 7: 681 Zhang B W. Mater Sci Eng. 2000; 281A: 286 Zhang B W. Acta Metall Sin. 1981; 17: 285
(张邦维. 金属学报,1981; 17:285)
[16]  Zhang H, Zhang B W, Wu L J, Wan Z Q. Physica, 1995; 205B: 263Zhang H, Zhang B W, Wu L J, Wan Z Q. Acta Phys Sm, 1994; 43:  1638
(张 恒,张邦维,吴力军,万志齐. 物理学报.1994;43:1638)
[17]  Niessen A K, Boer F R, Boom R. CALPHAD, 1983; 7: 51 
[18]  Smithells C J, Brandes E A. In:  Smithells C J ed., Metals Reference Book, 5th Edition, London:   Butterworths,1976:  100 
[19]  Marton J P, Schleshinger M. J Electrochem Soc, 1968; 16:234
[20]  Mallory G O. Plating, 1971; 58: 319 
[21] Chassaing E, Quang V K. Plat Surf Finish, 1990; 77: 60 
[22]  Schmeckenbecher A F. Plating, 1971; 58: 905 
[23] Zhang B W. Mech Eng Mater, 1988; 12(1): 30
(涨邦维. 机械工程材料,1988;12(1):30)
[24] Pan D, Turnbull D. J Appl Phys, 1974; 45: 1406
[25] Yan H. Shanghai Nonferous Met. 1994: 15: 294
(阎红.上海有色金属.1994;15:294)
[26]  Ruscior C, Croiala E. J Electrochem Soc, 1971; 118: 696 
[27] Hu W Y, Zhang B W. Physica, 1991; 175B: 396 
[28]  Chang Y S, Hsieh I J. Plat Surf Finish, 1990; 77; 52 
[29] Athavale S N, Totlani M K. Met Finish, 1989; 87: 23 
[30]  Koiwa I, Usuda M, Yamada K, Osaka T. J ElectrochemSoc, 1988; 135: 718 
[31] Zhang B W, Hu W Y, Qu X Y, Zhang Q L, Zhang H, TanZ S. Tram Inst Met Finish, 1996; 74: 69 
[32]  Cherkaoui M, Srhiri A, Chassaing E.  Plat Surf Finish,1992; 79: 68
[33] Si X L, Wu F, Zhu S Z. Funct Mater, 1995; 26:  189
(司秀丽.吴 丰.诸松竹.功能材料.1995:26:189)
[34]  Iwamatsu K. Met Finish, 1989; 87: 25 
[35] Kim D H, Matsuda H, Aoki K, Takano O. Sur/ Technol,1994; 45: 202 
[36] Gonzalez O M, White R E, Cocke D L. Plat Surf Finish,1990; 77: 63 
[37] El-Mallah A T, Abbas M H, Shafei M F, El-Sayed M,Hassan A, Nagi I, Borohydride P. Plat Surf Finish, 1989;76: 124 
[38] Hu W Y, Wang L L, Wu L J, Zhang B W, Guan H R.Trans Inst Met Finish, 1994; 72: 141 
[39]  Mallory G O, Horhn T R. Plat Surf Finish, 1979; 66: 40
[40]  Matsuoka M, Hayashi T. Plat Surf Finish, 1982; 69: 53 
[41]  Aoki K, Fukuda M, Takano O. Surf Technol,  1992; 43 ;857 
[42]  Wu Y X, Zhang J L. Plat Finish, 1998; 17:  11
(吴永析.张家乐 电镀与涂饰,1998 17:11)
[43]  Shipley C R Jr. Plat Surf Finish, 1984; 71: 92 
[44]  Kalu E E. Plat Surf Finish, 1998; 85: 74 
[45]  Schwartz M, Malloy G O. J Electrochem Soc, 1976; 123:606 
[46] Wang L L, Zhang B W, Yi G, Ouyang Y F, Hu W Y. JAlloys Compd, 1997; 255: 231 
[47] Wang L L, Zhao L H, Zhang B W, Shu X L, Sheng X,Fang Z Y. J Alloys Compd, 1999; 287: 234 
[48] Xie H W, Zhang B W, Yang Q Q. Trans Inst Met Finish,1999; 77: 99 
[49]  Yu G, Li Y J, Zhang N, Chen J X.   Weapons Mater SciEng, 1994; 17: 21
(于 光,黎永钧,张 楠,陈菊香 .兵器材料科学与工程,1994; 17:21)
[50]  Yang X J. Mater Protect, 1996; 29: 18
(杨贤金 材料保护,1996;29:18)
[51] Wang L L, Zhao L H, Huang G F, Yuan X J, Zhang B W.Surf Coat Technol, 2000; 126: 272 
[52] Wang L L, Zhao L H, Zhang B W, Liao S Z, Ouyang YF, Hu W Y. Z Metallkd, 1997; 88: 945 
[53]  Hung A, Hung P C, Ohno I. Plat Surf Finish, 1989; 76:60
[54]  Milad G, Mayes R. Met Finish, 1998; 96: 42 
[55]  Duncan G T, Banter J C. Plat Surf Finish, 1989; 76: 54 
[56]  Nawafune H, Uegaki T, Mizumoto S, Ishikawa M, Naka-mura T. Trans Inst Met Finish, 1998; 76: 231 
[57]  Zhang H, Zhang B W, Wu L J, Wan Z Q. Acta Phys, 1994;43: 1638 
[58]  Osaka T, Kasai N, Koiwa I, Goto F. J Electrochem Soc,1983; 130: 790 
[59] Yi G, Wang L L, Ouyang Y F, Mao L Y, Guo Y, ZhangB W, Xie H W. Met Finish, 1996; 94: 31
[1] 屈硕硕,祝清省,巩亚东,杨玉莹,李财富,高世安. 高浓度、高性能Pd胶体的制备及其活化机理[J]. 金属学报, 2017, 53(4): 487-493.
[2] 黄明亮,周少明,陈雷达,张志杰. Ni-P消耗对焊点电迁移失效机理的影响[J]. 金属学报, 2013, 49(1): 81-86.
[3] 李均明 薛晓楠 蔡辉 蒋百灵. 多孔结构MgO表面化学镀Ni层的制备与表征[J]. 金属学报, 2010, 46(9): 1103-1108.
[4] 王光君 王德志 周 杰 吴壮志 徐兵. Mo粉表面化学镀Cu及其反应机理[J]. 金属学报, 2009, 45(4): 405-409.
[5] 郭金明; 郭喜平; 宋曙光 . Nb-Ti-Si基多元合金在1250 ℃下的氧化行为[J]. 金属学报, 2008, 44(5): 574-578 .
[6] 蒋光锐; 刘源; 李言祥; 苏彦庆; 郭景杰 . 多元合金熔体组元活度系数计算方法的改进[J]. 金属学报, 2007, 43(5): 503-508 .
[7] 李钒; 张登君; 李报厚; 罗世民 . 六方BN微颗粒表面化学镀Ni及动力学模型[J]. 金属学报, 2004, 40(2): 173-178 .
[8] 郭忠诚. 稀土对复合镀工艺及镀层性能的影响[J]. 金属学报, 1996, 32(5): 516-520.
[9] 王正;张永升. Ni-P化学镀层对304钢应力腐蚀开裂的影响[J]. 金属学报, 1991, 27(2): 129-134.