| 氧对Mo-Si系机械合金化的影响 |
| 柳林 |
| 华中科技大学材料科学与工程学院模具技术国家重点实验室;武汉430074 |
|
引用本文:
柳林 . 氧对Mo-Si系机械合金化的影响[J]. 金属学报, 2001, 37(9): 1001-1004 .
[1] Koch C C, Cavin B, Mckamey C G, Scarbrough J O. ApplPhys Lett, 1983; 43. 1017 [2] Fecht H J, Han G, Fu Z, Johnson W L. J Appl Phys, 1990,67: 1744 [3] Liu L, Dong Y D. Nanostruc Mater, 1993, 2: 463 [4] Liu L, Chu Z Q, Dong Y D. J Alloy Compd, 1992; 186.217 [5] Yavari A R, Desre P J. Phys Reu Lett, 1990, 65: 2571 [6] Anton T, Liu Y, Parks T C, McCormick P G. Scr MetallMater, 1991; 25: 1607 [7] Anton T, Liu Y, Parks T C, McCormick P G. Scr MetallMater, 1992; 26. 1931 [8] Magini M, Padella F, Delogu P, Dikonimos T, Turtu S.Chem Mater, 1994; 6: 983 [9] Massalski T B, et al. eds. Binary Phase Diagram, ASMMetals Park, OH, 1986 [10] Iwamoto N, Uesake S. Mater Sci Forum, 1992; 88-90: 763 [11] Schwarz R B, Srinivasan S R, Petrovic J J, Maggiore C J.Mater Sci Eng, 1992; A155: 75 [12] Liu L, Magini M. J Mater Res, 1997, 12: 2281 [13] Doland C M, Nemanich R J. J Mater Res, 1990; 5: 2854 [14] Gasser R P H. An Introduction to Chemisorption andCatalysis by Metals, Oxford, United Kingdom: ClarendonPress, 1985 [15] Dobert C. Weast ed., Handbook of Chemistry and Physics,Boca Raton FL: CRC Press, 1988y |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|