| K40S合金高温时效过程中二次碳化物的沉淀析出行为 |
| 杨富民 孙晓峰 康煜平 管恒荣 胡壮麒 |
| 中国科学院金属研究所;沈阳110016 |
|
引用本文:
杨富民; 孙晓峰; 康煜平; 管恒荣; 胡壮麒 . K40S合金高温时效过程中二次碳化物的沉淀析出行为[J]. 金属学报, 2001, 37(3): 253-257 .
[1] lane J R, Grant N J. Trans ASM, 1952; 44: 113 [2] Sims C T. J Met, 1969; 21: 27 [3] Sims C T, Hagel W C. The Superalloys, New York: JohnWiley & Sons Inc., 1972: 145 [4] Jiang W H, Yao X D, Guan H R, Hu Z Q. Acta Met Sci,1999; 2(12): 155 [5] Jiang W H, Yao X D, Guan H R, Hu Z Q. Metall Trans,1999; 30A: 513 [6] Sims C T, Hagel W C. The Superalloys, New York: JohnWiley & Sons Inc, 1972: 115 [7] Jiang W H, Yao X D, Guan H R, Hu Z Q. J Mater SciLett, 1999; 18: 303 |
|