| Cr系白口铸铁动态相间腐蚀的定量研究 |
| 张安峰 邢建东 |
| 西安交通大学机械工程学院;西安710049 |
|
引用本文:
张安峰; 邢建东 . Cr系白口铸铁动态相间腐蚀的定量研究[J]. 金属学报, 2001, 37(1): 77-81 .
[1] Gahr K H Z, Eldis G T. Wear, 1980; 64: 175 [2] Parent S, Margerier J C. AFS Trans, 1972; 80: 393 [3] Gundlach R B. AFS Trans, 1974; 82; 309 [4] Dupin P, Saverna J, Schissler J M. AFS Trans,1982; 90:711 [5] Xing J D, Zhou Q D. AFS Trans, 1992; 100: 17 [6] Wu W Z, Xing J D, Su J Y. Acta Metall Sin, 1997; 33:1075(武文忠,邢建东,苏俊义.金属学报,1997;33:1075) [7] Pitt C H, Chang Y M. Corrosion, 1986; 42: 312 [8] Bronson A, Nelson J, Kang C. Wear, 1992; 154: 387 [9] Zhou Q D. Chromium Anti-Wear Cast Iron. Xi'an: Xi'anJiaotong University Publishing House, 1987: 102(周庆德.铬系抗磨铸铁.西安:西安交通大学出版社,1987:102) [10] Jiang X X, Wang J Y. Alloy Phase Electrochemistry.Shanghai: Shanghai Science and Technology PublishingHouse. 1984: 90(姜晓霞,王景蕴.合金相电化学.上海:上海科学技术出版社,1984:90) [11] Xu J. Corrosion Metal and Resist Corrosion Metal Material. Hangzhou: Zhejiang Science and Technology Publishing House, 1981: 129(徐 坚.腐蚀金属学及耐腐蚀金属材料.杭州:浙江科学技术出版社,1981:129) [12] Zhang A F, Xing J D, Gao Y M, Su J Y. Acta Metall Sin,2000; 36: 765(张安峰,邢建东,高义民,苏俊义.金属学报,2000;36:765) [13] Zhang A F, Xing J D, Gao Y M, Su J Y. J Xi'an JiaotongUniv, 2000; 34(9): 88(张安峰,邢建东,高义民,苏俊义.西安交通大学学报,2000;34(9):88) [14] Zheng Y G, Yao Z M, Wei X Y, Ke W. Wear, 1995; 186-187: 555` |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|