| 薄板坯连铸液芯铸轧过程的三维有限元分析 |
| 逯洲威 蔡开科 |
| 北京科技大学炼钢研究所; 北京 100083 |
|
引用本文:
逯洲威; 蔡开科 . 薄板坯连铸液芯铸轧过程的三维有限元分析[J]. 金属学报, 2000, 36(7): 757-760 .
[1] Yuan J H, Yu D L. Steelmaking, 1997; 13(2): 50(袁集华,于登龙.炼钢,1997;13(2:50) [2] Wunnenberg K, Schwerdtfeger K. Iron Steel Maker, 1995;22(4): 25 [3] Gosio G, Morando M, Manini L. Metall Plant Technol,1992; 15(2): 66 [4] Tian N Y. Thin Slab Continuous Casting and ContinuousRolling. Beijing: Metallurgical Industry Press, 1998: 60(田乃媛,薄板坯连铸连轧,北京:冶金工业出版社,1998:60) [5] Cremer B, Pawelski O, Rasp W. Ironmaking Steelmakiap,1993; 20: 264 [6] Gan Y, Chen D L. Iron Steel, 1999; 34(6): 27(干勇,陈栋梁,钢铁,1999;34(6):27) [7] Kelly J E, Michalek K P, O'connor T G, Thomas B J,Dantzig J A. Metall Trans, 1988; 19A: 2589 [8] Tszeng T C, Kobayashi S. Int J Mach Tools Manufact,1989; 29: 121 [9] Lu Z W, Cai K K, Zhang J Q. J Univ Sci Technol Beijing,1999. 21. 432(逯洲威,蔡开科,张家泉,北京科技大学学报,1999;21:432)^ |
|