| La2O3-Mo阴极表面碳化层作用机制研究 |
| 王金淑 周美玲 |
| 北京工业大学材料学院;北京 100022 |
|
引用本文:
王金淑; 周美玲 . La2O3-Mo阴极表面碳化层作用机制研究[J]. 金属学报, 2000, 36(11): 1205-1208 .
[1] Buxbaum C, Gessinger G. US Pat 4 019 081, 1977 [2] Buxbaum C, Gessinger G. US Pat 4 083 811, 1978 [3] Buxbaum C. Boveri Boveri Rev, 1979; 1:43 [4] Gessinger G, Buxbaum C. High Temp-High Pressures,1978; 10: 325 [5] Goebel D M, Forrester A T, Johnston S. Rev Sci Instrum,1980; 51: 1468 [6] Sreenivasa G R, Dharmadhikari C V, Nigavckar A S. JVac Sci Technol, 1989; A7: 3269 [7] Goebel D M, Barber G C. Rev Sci Instrum, 1985; 56: 1888 [8] Zhou M L, Chen Z C, Zhang J X. High Temp--High pressures, 1994; 26: 145 [9] Zhang J X, Zhou M L, Wang J S, Nie Z R, Zuo T Y. In:Xia Y T ed, '96 Symposium on Materials III-2, Beijing:Chemical Industry Press, 1996: 585(张久兴,周美玲,王金淑,聂祚仁,左铁镛.见:夏叶涛编,’96 中国材料研讨会III-2,北京:化学工业出版社,1996:585) [10] Nie Z R.Ph D Thesis, Central South University of Tech- nology, 1997 (聂祚仁.中南工业大学博士学位论文,1997) [11]Wang J S,Ph D Thesis,Beijing Polytechnic University, 1999 (王金淑.北京工业大学博士学位论文,1999) [12]Minanov X M,Hodakov I O C,Andosn T B,Markov M A ed. Liu H Q trans. Application of Rare Earth on Catalyst. Beijing:Science Press,1987:13 (Minanov X M, Hodakov I O C, Andosn T B, Markov M A著.刘恒潜译.稀土在催化中的应用.北京:科学出版社, 1987:13) [13] Zhou M L, Li J, Zuo T Y. Chin J Nonferrous Met, 1994; 4(2):45 (周美玲,李俊,左铁镛.中国有色金属学报,1994;4(2): 45) [14] Zhou M L, Li H G; Fu J F. Chin J Nonferrous Met, 1987; 6:11 (周美玲,李汉广,付炯芳.稀有金属材料与工程,1987; 6: 11)L |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|