| 非晶BCN的制备及其导电性 |
| 陈万金 华中 姚斌 刘力 苏文辉 丁炳哲 胡壮麒 |
| 吉林大学物理系; 长春 130023 |
|
引用本文:
陈万金; 华中; 姚斌; 刘力; 苏文辉; 丁炳哲; 胡壮麒 . 非晶BCN的制备及其导电性[J]. 金属学报, 1999, 35(5): 469-472 .
[1] Liu A Y, Cohen M L. Set, 1989; 245. 841 [2] Liu A Y, Wentzcovitch R M, Cohen M L. Phes Rev B, 1989,39B: 1760 [3] Badzian A R, Niemysky T, Olkusnik E. In:Glaski F Aed, Proceedings of the international Condrence on Chemical Vapor Deposition, Hinsdale, IL: American Nuclear, Society1972; 3: 747 [4] Watanabe M O, itch S, Mizushima K. i Appl Phal, 1995;78: 2880 [5] Pryor R A W. APPI Phes Lett, 1996; 68: 1602 [6] Kaner R B. Mater Res Bull, 1987, 22: 399 [7] Badzien A R. Mater Res Bull, 1981; 16: 1385 [8] Knittle E, Kanner R B, Jeanloz R, Cohen M L. Phal Red B,1995; 51B: 2149Z |
|