| 用含KBH4碱液处理改善M1Ni3.7Co0.6Mn0.4Al0.3贮氢合金电极的动力学性能 |
| 潘洪革 陈昀 陈长聘 王启东 |
| 浙江大学材料科学与工程系; 杭州 310027 |
|
引用本文:
潘洪革; 陈昀; 陈长聘; 王启东 . 用含KBH4碱液处理改善M1Ni3.7Co0.6Mn0.4Al0.3贮氢合金电极的动力学性能[J]. 金属学报, 1999, 35(3): 300-305 .
[1] Sakai T, Miyamura H, Kuriyama N, Kato A, Oguro K,Ishikawa H. J Electrochem Soc, 1990; 137: 795 [2] Willems J J G. Philips J Rearch, 1984; 39(Suupl.1): 1 [3] Sakai T,Oguru K, Miyamura H, Kuriyama N, Kato A,Ishikawa H. J Less-Cosmmon Met, 1990; 161: 193 [4] Suzuki K,Yanagihara N, Kawano H, Ohta A. J Alloys Comp,1993;s 192: 173 [5] Martin M,Gommel C, Borkhart C, Fromm E. J AlloysComa, 1996; 238: 193 [6] Furukawa N.J Power Sources, 1994; 51(1s-2): 45 [7] Ratnakumar B V, Witham C, Bowman R C, Hightower J A,Fultz B. J Electrochem Soc, 1996; 143: 2578 [8] Balasubramaniam R, Mungole M N, Rai K N. J AlloysComp, 1996; 196: 63 [9] Lichtenberg F,Kohler U, Fohler A, Adkins N J E, Zuttel A.J Alloys Comp, 1997; 253-254: 570 [10] Sakai T,Miyamura H, Kuriyama N, Kato A, Oguru K. JLess-Common Met, 1990; 159: 127 [11] Liu F,Suda S. J Alloys Comp, 1996; 232: 204 [12] Yan D Y,Suda S. J Alloyss Comp, 1995; 223: 28 [13] Ogawa H,Ikoma M, Kawano H, Matsumoto I. J PowerSources,1988; 12: 393 [14] Kuriyama N, Sakai T, Miyamura H, Tanaka H, Uehara I,Mell F, Schlapbach L. J Alloys Coma, 1996; 238: 128 [15] Iwakura C, Kim I, Matsui N, Inoue H, Matsuoka M. Electrochim Acta, 1993; 40: 659 [16] Mastsuoka M, Asai K, Fukumoto Y, Iwakura C. ElectrochimActa, 1995; 38: 561 [17] Wang C S, Let Y Q, Wang Q D. Electrochim Acta, 1998; 43:3193 [18] Notten P H L. Hokkeling P. J Electrochem Soc, 1991; 138.1877 [19] Zheng G, Popov B N, White R E. J Electrochem Soc, 1995;142: 2695 [20] Wang C S. J Electriochem Soc, 1998: 145: 1801 [21] Yang H W, Wang Y Y, Wan C C. J Electrochem Soc, 1996;143: 429 [22] Pan H G, Chen Y, Chen C P, Wang Q D. Eleatrochim Acta,Submitted |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|