| 有序和无序态Ni3Fe的环境氢脆研究 |
| 王松 万晓景 姚美意 |
| 上海大学材料研究所; 上海 200072 |
|
引用本文:
王松; 万晓景; 姚美意 . 有序和无序态Ni3Fe的环境氢脆研究[J]. 金属学报, 1999, 35(12): 1262-1265 .
[1] George E P, Liu C T, Pope D P. Scr Metall Mater 1993; 28:875 [2] Wan X J, Zhu J H, Jing K L. Scs Metall, 1992; 26: 473 [3] Takasugi T, Izumi O. Acta Metall, 1986; 34: 607 [4] Takasugi T, Izumi O, Yashida M. J Mater Sci, 1991; 26:1173 [5] Wan X J, Zhu J H, Jing K L, Chen W J, Wu Y. J Mater SciTechnol, 1994; 10: 39 [6] Liu C T, Lee E H, Mckamey C G. Scr Metall, 1989; 23: 875 [7] Wright J L, Zhu J H. Scr Mater, 1998; 38: 253 [8] Moms D G, Brown G T, Piller R C, Smallman R E. ActaMetall, 1976; 24. 21 [9] Zhu J H, S B Huang, Wan X J. Scr Metall Mater, 1995; 32:1399 [10] Wan X J, Cheng X Y, Chen Y X. Acta Metall Sin, 1998; 34:141(万晓景,程晓英.陈业新金属学报.1998;34:141) [11] Liu C T, Takeyama M. Scs Metall Mater, 1990; 24: 1583 [12] Takasugi T, Yoshida M. J Mater Sci, 1991; 26: 3032 [13] Takasugi T, Yoshida M. J Mater Res, 1985; 33: 1247 [14] Camus G M, Stoloff N S, Duquette D J. Acta Metall, 1989;37: 1497 [15] Takasugi T, Izumi O. Acta Metall, 1983, 31. 1187 [16] Kruisman J, Vitek V, Dehosson T M. Acta Metall, 1988; 36:2729 [17] Takasugi T, Hanada S. lutermetallics, 1994; 2: 225 [18] Su J Q, Gao S J, Zhang S S, Guo J T, Hu Z Q. Mater Lett,1997; 31: 227 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|