| XIE Youqing(Department of Materials Science and Engineering; Central South University of Technology; ChangSha 410083)CorrsPondent: XIE Youqing; pwtsson Tel: (O731)8879287; Fax: (0731)8826136Manuscript received 1997-12-1; in revised form 1998-0406 |
引用本文:
谢佑卿. Cu-Ni合金组元的偏原子体积与平均原子体积的关系[J]. 金属学报, 1998, 34(12): 1243-1248.
.
RELATIONSHIP BETWEEN PARTIAL AND AVERAGE ATOMIC VOLUMES OF COMPONENTS IN Cu-Ni ALLOYS[J]. Acta Metall Sin, 1998, 34(12): 1243-1248.
1谢佑卿.中国科学,1997;E27:488(Xie Y Q.SCi Chin,1998; E41:146) 2谢佑卿,张晓东中国科学,1998;E28:12(Xie Y Q, Zhang X D. Sci Chin, 1998; E41: 157) 3 Walter J M. Physical Chemistry London: Longman Group Limited; 1976: 230 4谢佑卿,张晓东金属学报,1994;A30:531(Xie Y Q, Zhang X D. Acta Metall Sin, 1994; A30: 531) 5谢信卿,马柳莺,张晓东等.中国科学,19932 A23:999(Xie Y Q, Ma L Y, Zhang X D et al. Sci Chin, 1993; A36: 612) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|