| 两相材料的弹塑性性质和计算模型分析 |
| 周喆;匡震邦 |
| 北方交通大学;北京;100044;上海交通大学;上海;200030 |
|
| ANALYSIS OF THE ELASTO-PLASTIC PROPERTIES AND COMPUTATIONAL MODELS FOR TWO-PHASE COMPOSITES |
| ZHOU Zhe(Northern Jiaotong University; Beijing 100044); KUANG Zhenbang (Shanghai Jiaotong University); Shanghai 200030) |
引用本文:
周喆;匡震邦. 两相材料的弹塑性性质和计算模型分析[J]. 金属学报, 1997, 33(9): 903-911.
,
.
ANALYSIS OF THE ELASTO-PLASTIC PROPERTIES AND COMPUTATIONAL MODELS FOR TWO-PHASE COMPOSITES[J]. Acta Metall Sin, 1997, 33(9): 903-911.
1Eshelby J D.Proc roy soc,1957;A241:376 2Hill R.J.Mech Phys Solids,1965;13:213 3Mori T,Tanaka K.Acta metall ,1973;21:571 4Tandon G P,Weng G J Appl Mech 1988;55:126 5Shen Y L ,Finot M,Needleman A,Suresh S.Acta Metall Mater,199443:1701 6Dutta I,Sims J D,Seigenthaler D M.Acta Metall Mater,1993;41:885 7Smith J D.J Res National Bureau Standard 1974 78A: 355 8匡震邦.非线性连续介质力学基础西安:西安交通大学出版社,1989:140 |
|