| 水平电磁连铸中金属磁悬浮行为 |
| 任忠鸣;周月明;张春源;蒋国昌 |
| 上海大学;上海市钢铁冶金新技术开发应用重点实验室 |
|
| LEVITATION BEHAVIOUR OF METAL IN HORIZONTAL ELECTROMAGNETIC CONTINUOUS CASTING |
| REN Zhongming; ZHOU Yueming; ZHANG Chunyuan; JIANG Guochang (Shanghai University; Shanghai Enhanced Laboratory of Ferroumetallurgy; Shanghai 200072) |
引用本文:
任忠鸣;周月明;张春源;蒋国昌. 水平电磁连铸中金属磁悬浮行为[J]. 金属学报, 1996, 32(6): 642-646.
,
,
,
.
LEVITATION BEHAVIOUR OF METAL IN HORIZONTAL ELECTROMAGNETIC CONTINUOUS CASTING[J]. Acta Metall Sin, 1996, 32(6): 642-646.
| 1小冢敏之,浅井滋生.鞭岩.铁钢.1988:74:17932浅井滋生,小冢敏之,鞭岩.铁钢,1986:72:22183TakeuchiS,EtayJ,GarnierM.ISIJInt,1989;29:10064HullJR,LariRJ,PraegWF,TurnerLR.USPat,4678024,19875YoshidaM,InumaruS.USPat.4694888,19876LaversJD.In:IEEE-IASed.,IEEE-IASConfProc,SanFransisco:IEEE-IndustryApplicationSociety,1982:9547任忠鸣,范江虹.中国有色金属学报,1993;3(2):93 |
|