| 钇对超微晶软磁合金结构和磁性能的影响 |
| 马如璋;刘涛;陈菊芳;杨国斌;徐祖雄;顾红霞 |
| 北京科技大学 |
|
| EFFECT OF YTTRIUM ADDITION ON MICROSTRUCTURE AND MAGNETIC PROPERTIES OF NANOCRYSTALLINE SOFT MAGNETIC ALLOY |
| MA Ruzhang; LIU Tao; CHEN Jufang; YANG Guobin; XU Zuxiong; GU Hongxia(University of Science Technology Beijing; Beijing 100083)(Manuscript received 1995-05-19) |
引用本文:
马如璋;刘涛;陈菊芳;杨国斌;徐祖雄;顾红霞. 钇对超微晶软磁合金结构和磁性能的影响[J]. 金属学报, 1996, 32(2): 207-210.
,
,
,
,
,
.
EFFECT OF YTTRIUM ADDITION ON MICROSTRUCTURE AND MAGNETIC PROPERTIES OF NANOCRYSTALLINE SOFT MAGNETIC ALLOY[J]. Acta Metall Sin, 1996, 32(2): 207-210.
| 1YoshizawaY,OgumaS,YamauchiK.JApplPhys,1988;64:60442YoshizawaY,YamauchiK.IEEETransMag,1989;25:33253HerzerG.IEEETransMag,1989:25:33234HonoK,InoueA,HonoK,InoueA,SakuraiT.ApplPhysLett,1993;58:21805徐祖雄,徐震东,杨会生,马如璋.科学通报,1993;38:5126StearnMB.PhysRev,1963;129:11367顾红霞,北京科技大学硕士论文,1994t |
|