| 弥散CeO_2对高温下α-Al_2O_3氧化膜初期生长的影响 |
| 马信清;李美栓;彭晓;陈全芳;李铁藩 |
| 中国科学院金属腐蚀与防护研究所腐蚀与防护国家重点实验室 |
|
| EFFECT OF CeO_2 DISPERSION ON INITIAL STAGE GROWTH OF α-Al_2O_3 OXIDE SCALE AT HIGH TEMPERATURE |
| MA Xinqing; LI Meishuan; PENG Hiao; CHEN Quanfang; LI Tiefan (State Key. Laboratory; of Corrosion and Protection; Inslitute of Corrosion and Prolection of Metals;Chinese Academy; of. Sciences; Shenyang 110015)(Manuscript received 1995-01-10; in revised form 1995-06-06) |
引用本文:
马信清;李美栓;彭晓;陈全芳;李铁藩. 弥散CeO_2对高温下α-Al_2O_3氧化膜初期生长的影响[J]. 金属学报, 1995, 31(21): 399-405.
,
,
,
,
.
EFFECT OF CeO_2 DISPERSION ON INITIAL STAGE GROWTH OF α-Al_2O_3 OXIDE SCALE AT HIGH TEMPERATURE[J]. Acta Metall Sin, 1995, 31(21): 399-405.
| 1HindamH,WhittleDP.OxidMet、1982:18:2452whittleDP.StringerJPhilosTransRSocLond,1980:A295:3093WagnerC.CorroSci,1965:5,7514StringerJ,WilcoxBA,JaffeeRI.OxidMet1972;5:115KvernesIA.OxidMet1973:6,456FlowerHM.WilcoxBA.CorroSci,1977:12,2437MoulinP,HuntzAM,BerangerG,LacombeP.SerMetall.1977:11:5338李铁藩,马信清,金属学报,1991;21:B259NagaiH.JJapanInstMet,1981;22:10110HouPY.StringerJJElectrochemSoc,1987:134,193611WahlG.ThinSolidFilms,1983:107:41712WangG,GleesonB,DouglassDL.Oxidmet.199135:33313WallworkGR,HedAZ.oxidmet,1971;3:17114郭大钧,大学数学手册.济南:山东科学出版社,1985:174 |
|