| 机械球磨制备Fe纳米晶及其Mossbauer效应 |
| 陈洪;徐祖雄;翟少岩;马如璋 |
| 北京科技大学 |
|
| MoSSBAUER EFFECT ON BALL-MILLED NANOCRYSTALLINE Fe MATERIALS |
| CHEN Hong; XU Zuxiong; ZHAI Shaoyan; M A Ruzhang(University of Science and Technology Beijing; 100083)(Manuscript received 94-03-16; in revised form 94-08-16) |
引用本文:
陈洪;徐祖雄;翟少岩;马如璋. 机械球磨制备Fe纳米晶及其Mossbauer效应[J]. 金属学报, 1995, 31(14): 73-76.
,
,
,
.
MoSSBAUER EFFECT ON BALL-MILLED NANOCRYSTALLINE Fe MATERIALS[J]. Acta Metall Sin, 1995, 31(14): 73-76.
| 1BirringerR,GleiterH,KleinHP,MarquardtP.PhysLett,1984;102A:3652HellU,JingJ,BirringerR,GonserU,GleiterH.ApplPhysLett,1987;50:4723SchaeferHE,WurschumR.PhysLett,1987;A119:3704YangYZ,MaXM,DongYD,HeYZ,WangGM.ChinesePhysLett,1992;9:2665FechtHJ,HerllsternE,FuZ,JonsonWL.MetallTrans,1990;21A:23336DavisRM,McDermottB,KochCC.MetallTrans,1988;19A:28677TrudeauML,SchultzR.MatSciEng,1991;A1338EL-EskandaranyMS,SumiyamaK,AokiK,SizukiK.JMaterRes,1992;7:8889RonM.ApplicationofMssbauerSpectroscopy,Vol.2,NowYork,AcademicPress,1980,329 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|