| Ⅰ+Ⅱ复合型载荷缺口前端双氢峰规律的研究 |
| 王利;陈廉 |
| 中国科学院金属研究所;辽宁省材料与氢重点实验室;上海宝山钢铁(集团)公司钢铁研究所 |
|
| DOUBLE PEAK OF HYDROGEN ACCUMULATION NEAR NOTCH TIP UNDER Ⅰ+Ⅱ LOADING MODE |
| WANG Li; CHEN Lian(Institute of Metal Research; Chinese Academy of Sciences;Liaoning Key Laboratory for Materials and Hydrogen;Shenyang 110015)(Manuscript recieved 1994-06-25; in revised form 1995-01-16) |
引用本文:
王利;陈廉. Ⅰ+Ⅱ复合型载荷缺口前端双氢峰规律的研究[J]. 金属学报, 1995, 31(10): 461-468.
,
.
DOUBLE PEAK OF HYDROGEN ACCUMULATION NEAR NOTCH TIP UNDER Ⅰ+Ⅱ LOADING MODE[J]. Acta Metall Sin, 1995, 31(10): 461-468.
| 1TroianoAR.TransASM,1960;52:542OchiaiS,YoshinagaS,KikutaY.TransIronSteelInstJpn,1975,15:5033YamakawaK,YonezawaS,YoshizawaS.MetallicCorrosion,Int.Congress,Vo1.2,CanadaToronto,1984:25441982;(6):1025RobinsonSL,MoodyNR,CostaJC,PontauAE,GerberichWW.ScrMetall,1990;24:1116Wushiding,ChenLian,LiuMinzhi.ActaMetallSinica,1990;3:3127LiYiyi,MaLuming,LiangGuojun.ChinJMetSciTechnol,1987;3:748SihGC.EngFractMech,1973;5:3659王利,陈廉.分析仪器,1994;(3):910BatheKJ著,张圣坤,韩继文,汪庠宝,杨文华译校,非线性有限元分析ADINA理论文本.上海交通大学科技交流室,198611ChenXiaolie,NakasaKeijiro,EngFractMech,1989;33:13312LiJCM,OrianiRA,DarkenLS.ZPhysChem,1966;49:271P |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|