| 粗糙度引入的Ⅱ型裂纹扩展的剪切阻力 |
| 郑冶沙;王中光;艾素华 |
| 中国科学院上海硅酸盐研究所;博士后;上海200050;中国科学院金属研究所材料疲劳与断裂国家重点实验室;中国科学院金属研究所材料疲劳与断裂国家重点实验室 |
|
| ROUGHNESS-INDUCED SHEAR RESISTANCE OF MODE Ⅱ CRACK GROWTH |
| WANG Zhongguang;AI Suhua State Key Laboratory of Fatigue and Fracture for Materials; Institute of Metal Research; Academia Sinica; ShenyangZHENG Yessha;post-doctoral.Shanghai Institute of Coramics.Academia Sinica.Shnaghai 300050 |
引用本文:
郑冶沙;王中光;艾素华. 粗糙度引入的Ⅱ型裂纹扩展的剪切阻力[J]. 金属学报, 1993, 29(6): 13-21.
,
,
.
ROUGHNESS-INDUCED SHEAR RESISTANCE OF MODE Ⅱ CRACK GROWTH[J]. Acta Metall Sin, 1993, 29(6): 13-21.
1 Gao H, Brown M W, Miller K J. Fatigue Engng Mater Struct, 1982; 5 (1) : 117 2 Wang K J, Hsu C L, Kao H. Proc I CFA, 1977; 4: 123--133. Pergamon press. 3 Gao H, Wang Z, Yang C, Zhou Z. Acta Metall. Sin, 1979; 15: 380--391. 4 Maccagno T M, Knott J F. Engng Fract Mech, 1989; 34 (1) : 65--86 5 Tanaka K. Engng Fract Mech, 1974; 6: 493 6 Liu H W. Fatigue Fract Engng Mater Struct, 1985; 8 (4) : 295--313 7 Gough H J. Edgar Margurg Lecture, Proc. ASTM 1133; 33 (part Ⅱ): 111. 8 Erdogan F, Sih G C. J Basic Engng (ASME Trans), 1963; 85: 519--527 9 K Hyashi, Nemat-Nasser S. J Appl Mech, 1981; 48: 520. 10 Sih G C. Int J Fracture, 1974: 10: 305--321. 11 Brown M W, Liu H W, Kfouri A P, Miller K I. Proc ICF5, 1980; 12: 891. Pergamon Press.R |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|