| PbCl_2-NaCl-BaCl_2三元熔盐的混合焓 |
| 于化龙;竺建康;王之昌 |
| 东北工学院;东北工学院;东北工学院;教授;沈阳(110006)东北工学院有色冶金系 |
|
| ENTHALPIES OF MIXING FOR PbCl_2-NaCl-BaCl_2 TERNARY MOLTEN SALT MIXTURES |
| YU Hualong;ZHU Jiankang;WANG Zhichang Northeast University of Technology; Shenyang Correspondent; professor; Department of Non-Ferrous Metallurgy; Northeast University of Technology; Shenyang 11006 |
引用本文:
于化龙;竺建康;王之昌. PbCl_2-NaCl-BaCl_2三元熔盐的混合焓[J]. 金属学报, 1992, 28(5): 90-92.
,
,
.
ENTHALPIES OF MIXING FOR PbCl_2-NaCl-BaCl_2 TERNARY MOLTEN SALT MIXTURES[J]. Acta Metall Sin, 1992, 28(5): 90-92.
1 Sommer F. J Thermal Anal, 1988; 33: 15 2 Moser Z, Gasior W, Sommer F, Schwitzgebel G, Predel B. Metall Trans, 1986; 17B: 791 3 Kubaschewski O, Alcock C B. Metallurgical Thermochemistry. 5th ed., New York: Pergamon, 1979 4 Hino M, Kelly M G, Toguri J M. Can Metall Q, 1990; 29: 177 5 Barton J L, Bloom H. J Phys Chem, 1956; 60: 1413 6 McCarty F G, Kleppa O J. J Phys Chem, 1964; 68: 3846 7 Barin I, Knacke O. Thermochemical Properties of Inorganic Substances. Berlin: Springer Verlag, 1973 8 Hassam S, Gaune-Escard M, Bros J P, Hoch M. Metall Trans, 1988; 19A: 2075 9 Tian Y W, Yu H L, Zhang X H, Zhu J K, Wang Z C. J Phys Chem, to be submitted 10 王之昌.金属学报,1982;18:141v |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|