铁基合金马氏体的形核与长大 |
张修睦;李依依 |
中国科学院金属研究所;中国科学院金属研究所 |
|
NUCLEATION AND GROWTH OF FERROUS MARTENSITES |
ZHANG Xiumu;LI Yiyi Institute of Metal Research; Academia Sinica; Shenyang |
引用本文:
张修睦;李依依. 铁基合金马氏体的形核与长大[J]. 金属学报, 1991, 27(3): 19-26.
,
.
NUCLEATION AND GROWTH OF FERROUS MARTENSITES[J]. Acta Metall Sin, 1991, 27(3): 19-26.
1 Olson G B, Cohen M. Metall Trans, 1976; 7A: 1897--1915 2 蒋生蕊,金属学报,1986;22:A393;1988;24(增刊Ⅰ):A 40 3 Zhang X M, Gautier E, Simon A. Acta Metall, 1989; 37: 487 4 Kajiwara S. Metall Trans, 1986; 17A: 1693 5 Schumann H. Prakt Metallogr, 1975; 12: 511 6 Shimizu K, Tanaki T. Trans Jpn Inst Met, 1978; 19: 685 7 Brooks J W, Lorotto M H, Smallmann R E. Acta Metall, 1979; 27: 1839 8 Zhang Xiumu, Li Yiyi, Chen Lang, Li Hengwu. ICOMAT-86, Nara, Japan, 1986, Japan Inst Metals, 1987: 482 9 Sleeswyk A W. Acta Metall, 1962; 10: 705 10 Kakesnita T, Shimizu K, Maki T, Tamura I. Scr Metall, 1980; 14: 1067 11 Sadovsky V D. Proc ICOMAT-86, Nara. Japan, 1986, Japan Inst Metals, 1987. 222 12 Okamoto H, Oka M. Proc ICOMAT-86, Nara, Japan, 1986, Japan Inst Metals, 1987: 276 13 Zhang X M, Zhao X, Zhong J X, Qi Y. Scr Metall, 1990; 24: 1594 14 Wen Youhai, Zhang Xiumu, Zhao Xu, Li Yongsen. Chin J Met Sci Technol, 1991; 7(3) : 211 15 Zhao X, Zhang X M, He Y Y, Li B. Cryogenics, 1990; 30: 404 16 Gong H, Zhang X M. Mater Forum, 1990; 14: 137--141 17 贡海,章为夷,张修睦.金属学报,1991;27(3) :A201 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|