| BaB_2O_4-BaF_2相图的测定和计算 |
| 饶光辉;乔芝郁;梁敬魁 |
| 中国科学院物理研究所;北京科技大学;副教授;中国科学院物理研究所 |
|
| MEASURED AND CALCULATED BaB_2O4-BaF_2 BINARY PHASE DIAGRAM |
| RAO Guanghui Institute of Physics; Academia Sinica; Beijing; QIAO Zhiyu University of Science and Technology Beijing; LIANG Jingkui Institute of Physics; Academia Sinica; Beijing |
引用本文:
饶光辉;乔芝郁;梁敬魁. BaB_2O_4-BaF_2相图的测定和计算[J]. 金属学报, 1991, 27(2): 145-147.
,
,
.
MEASURED AND CALCULATED BaB_2O4-BaF_2 BINARY PHASE DIAGRAM[J]. Acta Metall Sin, 1991, 27(2): 145-147.
1 Levin E M, McKurde H F. J Res Nat Bur Stard, 1949; 42: 131 2 梁敬魁,张玉苓,黄清镇.化学学报,1982;40:994 3 王国富,黄清镇.物理学报,1985;34:562 4 Rao G H, Liang J K. Qiao Z Y, Huang Q Z. CALPHAD, 1989; 13: 169 5 黄清镇,梁敬魁.物理学报,1981;30:559 6 JANAF Thermodynamical Tables (Supplement Vol. 1974, 1975, 1978) , Tokyo, 1977 7 乔芝郁,王明生,郑朝贵,段淑贞.中国稀土学报,1989;7(4) :16 8 饶光辉.中国科学院物理研究所博士论文,198 |
|