| 4Cr5MoV1Si(H13)钢合金氮化物的形貌和晶体学特征 |
| 罗承萍;赵方 |
| 华南理工大学机械二系;副教授;华南理工大学 |
|
| MORPHOLOGY AND CRYSTALLOGRAPHY OF ALLOY NITRIDES IN DIFFUSIONAL NITRIDED LAYER OF 4Cr5MoVlSi STEEL |
| LUO Chengping;ZHAO Fang South China University of Technology; Guangzhou |
引用本文:
罗承萍;赵方. 4Cr5MoV1Si(H13)钢合金氮化物的形貌和晶体学特征[J]. 金属学报, 1990, 26(6): 34-39.
,
.
MORPHOLOGY AND CRYSTALLOGRAPHY OF ALLOY NITRIDES IN DIFFUSIONAL NITRIDED LAYER OF 4Cr5MoVlSi STEEL[J]. Acta Metall Sin, 1990, 26(6): 34-39.
1 Phillips V A, Seybolt A U. TMS AIME, 1968; 242: 2415 2 Jack K H. Heat Treatment'73, London: The Metals Society, 1973: 39 3 郑经紘,王育烽,沈甫法,俞德刚,毛树楷.金属学报,1985;21:A333 4 Hirsch P, Howie A, Nicholson R B, Pashley D W, Whelan M J. Electron Microscopy of Thin Crystals, Malabar, Florida: Krieger R E Publishing Company, 1977: 320 5 #12 6 Dahmen U. Acta Metall, 1982; 30: 63 7 Luo C P, Weatherly G C. Acta Metall, 1987; 335: 1963 8 Aaronson H I, Laird C, Kinsman K R. Phase Transformations, Metal Park, Ohio: ASM, 1970: 313 |
|