| 解理裂缝过界扩展模型 |
| 黄正;姚枚 |
| 中国科学院物理研究所;北京(100080);哈尔滨工业大学 |
|
| MODEL OF CLEAVAGE CRACK PROPAGATION ACROSS BOUNDARY |
| HUANG Zheng;YAO Mei Institute of Physics; Academia Sinica; Beijing Harbin Institute of Technology Institute of Physics;Academia Sinica;Beijing 100080 |
引用本文:
黄正;姚枚. 解理裂缝过界扩展模型[J]. 金属学报, 1990, 26(1): 53-57.
,
.
MODEL OF CLEAVAGE CRACK PROPAGATION ACROSS BOUNDARY[J]. Acta Metall Sin, 1990, 26(1): 53-57.
1 Knott J F. Philips Trans R Soc, London, 1981; 229A: 45 2 Qu D, Wang X W, Tsai C K. In: Carlsson J, Chalson N G eds., Mechanical Behaviour of Materials-IV, Vol. Ⅱ, Oxford: Pergamon, 1984: 779 3 Lin T, Evans A G, Ritchie R O. Metall Trans, 1987; 18A: 641 4 Yao M, He Y K, Li D M, Zhou C Z. In: Vallari S R, Taplin D M, Roma Rao P, Knott J F, Dukey R eds., Advances in Fracture Research (Fracture 84) . Vol. Ⅱ, Oxford: Pergamon. 1984; 2: 1423 5 姚枚,何裕宽,李道明,钢铁,1984;19(12) :10 6 黄正,姚枚,金属学报,1988;24(增刊Ⅰ):96 7 Hahn G T, Gibert A, Reid C N. J Iron Steel Inst, 1964; 202: 677 8 黄正.哈尔滨工业大学博士学位论文,1987 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|