| Fe-Cr-Mo三元系高温区的金属间化合物及其生成反应 |
| 刘世程;浜口由和;桑野寿 |
| 大连铁道学院热处理教研室;讲师;日本室兰工业大学;日本室兰工业大学 |
|
| INTERMETALLIC COMPOUNDS AND THEIR FORMATION REACTIONS IN HIGH-TEMPERATURE REGION OF Fe-Cr-Mo SYSTEM |
| LIU Shicheng;HAMAGUCHI Yoshikazu;KUWANO Hisashi Dalian Railway Institute Muroran Institute of Technology; Japan |
引用本文:
刘世程;浜口由和;桑野寿. Fe-Cr-Mo三元系高温区的金属间化合物及其生成反应[J]. 金属学报, 1989, 25(2): 109-115.
,
,
.
INTERMETALLIC COMPOUNDS AND THEIR FORMATION REACTIONS IN HIGH-TEMPERATURE REGION OF Fe-Cr-Mo SYSTEM[J]. Acta Metall Sin, 1989, 25(2): 109-115.
1 Wada T. Metals Handbook, 8th ed., Vol. 8: Metallography Structures and Phase Diagiams, ASM, 1973: 421 2 Raynor G V. Rivlin V G. Int Metall Rev, 1984; 29 (5) : 329 3 Sinha A K. Buckley R A. Hume-Rothery W. J Iron Steel Inst, London, 1967; 205: 191 4 武田修三,汤川夏夫.日本金属学会志,1957;21:275 5 Bechtoldt C J, Vacher H C. J Res Nat Bur Stand, 1957; 58: 7 6 Goldschmidt H J. Iron and Steel Inst, Special Report, №43, 1951: 249 7 Goldschmidt H J. Trans ASM, 1954; 46: 807 8 Goldschmidt H J. Metallurgia, 1957; 56: 17 9 高武盛,西沢泰二.日本金属学会志,1979;43:118 10 Komura Y, Sly W G. Shoemaker D P. Acta Crystallogr, 1960; 13: 575 11 刘世程.日本东北大学博土论文,1987 12 Dyson D J, Keown S R. Acta Metall, 1969; 17: 1096 13 Hughes H, Keown S R. J Iron Steel Inst, London, 1968; 206: 275 14 VerSnyder F L, Beattie H J Jr. Trans ASM, 1955; 47: 212 15 McMullin J G, Reiter S F, Ebeling D G. Trans ASM, 1954; 46: 799 |
|