| 铸锭旋转对宏观偏析的影响 |
| 喻秋平;周尧和 |
| 西安市西北工业大学403教研室;西北工业大学 |
|
| INFLUENCE OF MOULD ROTATION ON MACROSEGREGATION IN INGOT |
| YU Qiuping;ZHOU Yaohe Northwestern Polytechnical University; Xi'an |
引用本文:
喻秋平;周尧和. 铸锭旋转对宏观偏析的影响[J]. 金属学报, 1988, 24(5): 379-384.
,
.
INFLUENCE OF MOULD ROTATION ON MACROSEGREGATION IN INGOT[J]. Acta Metall Sin, 1988, 24(5): 379-384.
1 Kirkaldy J S, Youdelis W V. Trans Metall Soc AIME, 1958; 212: 833--840 2 Mehrabian R, Keane M, Flemings M C. Metall Trans, 1970; 1: 1209--1220 3 McDonald R J. Hunt J D. Trans Metall Soc AIME, 1969; 245: 1993--1997 4 Stewart M J, MacAulay L C. Weinberg P. Metall Trans, 1971; 2: 169--173 5 Kou S, Poirier D R Flemings M C. Metall Trans 1978; 9B: 711--719 6 Moore J J, Shah N A. Int Metall Rev, 1983; 28: 338--356 7 喻秋平,枝晶间液相流动与宏观偏析,西北工业大学科技资料,CL8613,1986 |
|