    					| 用CBED测定PrCo_(12)B_6化合物的空间群 | 
  					 
  					  										
						| 王福会;边为民 | 
					 
															
					| 沈阳中国科学院金属腐蚀与防护研究所;东北工学院 | 
					 
										
						 | 
					 
   										
    					| DETERMINATION OF SPACE GROUP OF PrCo_(12)B_6 COMPOUND BY COVERGENT BEAM ELECTRON DIFFRACTION | 
  					 
  					  					  					
						| WANG Fuhui;BIAN Weimin Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang; Northeast University of Technology; Shenyang | 
					 
														 
				
				引用本文: 
				
								王福会;边为民. 用CBED测定PrCo_(12)B_6化合物的空间群[J]. 金属学报, 1988, 24(4): 368-370.	
																												 																				 ,
																												 . 
				DETERMINATION OF SPACE GROUP OF PrCo_(12)B_6 COMPOUND BY COVERGENT BEAM ELECTRON DIFFRACTION[J]. Acta Metall Sin, 1988, 24(4): 368-370.	                                                        				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
                         
            
									            
									                
																														  
																  1 Niinara K, Yajima S, Chem Lett, 1972; (10) : 875 2 #12 3 ElMasry N A, Stadelmaier H H. J Less-Common Met, 1984; 96: 165 4 Chuang Y C, Wu C H, Wang F H. J Less-Common Met, 1987; 135: 5 5 Hahn T. International Tables for Crystallography, Vol. A, Holland, Boston: Reidel, 1983: 534 6 Buxton B F, Eades J A, Steeds J W, Raokham G M. Philos Trans Roy Soc London, Ser. A1976; 281: 171 7 Tanaka M, Saito R, Sekii H, Acta Crystallogr, 1983; A39: 357 | 
															   
																													 
									             
									           
             
			            			 
			 
             
												
											    	
											        	 | 