| 零电阻温度85.3K的Bi系氧化物超导体 |
| 史凡;周寿增;史振华;李佛标 |
| 北京钢铁学院材料科学与工程系;北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| Bi-Sr-Ca-Cu OXIDE SUPERCONDUCTOR WITH ZERO RESISTANCE TEMPERATURE 85.3K |
| SHI Fan;ZHOU Shouzeng;SHI Zhenhua;LI Fubiao Beijing University of Iron and Steel TechnologyDepartment of Materials Science and Engineering;Beijing University of Iron and Steel Technology; Beijing |
引用本文:
史凡;周寿增;史振华;李佛标. 零电阻温度85.3K的Bi系氧化物超导体[J]. 金属学报, 1988, 24(4): 371-372.
,
,
,
.
Bi-Sr-Ca-Cu OXIDE SUPERCONDUCTOR WITH ZERO RESISTANCE TEMPERATURE 85.3K[J]. Acta Metall Sin, 1988, 24(4): 371-372.
1 Michel C, Hervieu M, Borel M M. Grandin A, Deslandes F, Provost J, Raveau B. Z Phys B, 1987; 68: 421 2 Maeda H, Tanaka Y, Fukutomi M, Asano T. Jpn. J Appl Phys Part 2 Lett, 1988 |
|