| 非晶(Fe_(80)Ni_(20))_(78)Si_(22-x)B_x合金的磁矩与Curie温度 |
| 官可洪;卜晓东 |
| 东北工学院材料科学与工程系;东北工学院 |
|
| MAGNETIC MOMENT AND CURIE TEMPERATURE OF (Fe_(80)Ni_(20))_(78)Si_(22-x)B_x AMORPHOUS ALLOYS |
| GUAN Kehong;PU Xiaodong Northeast University of Technology; ShenyangDept. Mater. Sci.; Northeast University of Technology;Shenyang |
引用本文:
官可洪;卜晓东. 非晶(Fe_(80)Ni_(20))_(78)Si_(22-x)B_x合金的磁矩与Curie温度[J]. 金属学报, 1988, 24(3): 296-298.
,
.
MAGNETIC MOMENT AND CURIE TEMPERATURE OF (Fe_(80)Ni_(20))_(78)Si_(22-x)B_x AMORPHOUS ALLOYS[J]. Acta Metall Sin, 1988, 24(3): 296-298.
1 Ward K D, Crangle J, Davies H A. In: Masumoto T et al. eds. The Magnetic Moments on Fe, Co and Ni Atoms in Amorphous Alloys Containing Boron, Proc 4th Int Conf on Rapidly Quenched Metal, Sendai. Aug 24--28, 1981, Japan: The Japan Institute of Metals, 1982: 1141--1144 2 Kaneyoshi T. In: Hasegawa R ed., Magnetic Chemical and Structural Properties in Glass Metallic Alloys, Cleveland, Ohio: Chemical Rubber Co., 1981: 38--409 |
|