| Nd-Fe-B磁体杨氏模量随温度的变化 |
| 罗阳;张宁 |
| 高级工程师;北京学院南路76号冶金工业部钢铁研究总院精密合金部;冶金工业部钢铁研究总院 |
|
| VARIATION OF YOUNG'S MODULUS WITH TEMPERATURE IN Nd-Fe-B MAGNET |
| LUO Yang;ZHANG Ning Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; BeijingSenior Engineer;Dept. of precision Alloys Central Iron and Steel Research Institute;Ministry of Metallurgical Industry;Beijing |
引用本文:
罗阳;张宁. Nd-Fe-B磁体杨氏模量随温度的变化[J]. 金属学报, 1988, 24(3): 293-295.
,
.
VARIATION OF YOUNG'S MODULUS WITH TEMPERATURE IN Nd-Fe-B MAGNET[J]. Acta Metall Sin, 1988, 24(3): 293-295.
1 罗阳,张宁.金属学报,1987;23(1) :A95 2 高占武.高温弹性模量测量新技术,1983;未发表 3 Luo Yang, Ning Zhang. Graham C D Jr. J Appl Phys, 1987; 61(8) : 3442 4 Glvord D, Li H S, Morean J M, Tenaud P. J Magn Magn Mater, 1986; 54--57: 445 5 Lee R W, Schaffel N, Brewer E G. IEEE Trans Magn, 1985; MAG-21: 195 |
|