| Al_2O_3对镁铬耐火材料在炉外精炼渣中溶蚀的影响 |
| 陈肇友;刘波 |
| 高级工程师;冶金工业部洛阳耐火材料研究所;冶金工业部洛阳耐火材料研究所 |
|
| INFLUENCE OF Al_2O_3 ON DISSOLUTION OF MAGNESITE-CHROME REFRACTORY IN STEEL REFINING SLAG |
| CHEN Zhaoyou;LIU Bo Luoyang Institute of Refractories Research; Ministry of Metallurgical Industry |
引用本文:
陈肇友;刘波. Al_2O_3对镁铬耐火材料在炉外精炼渣中溶蚀的影响[J]. 金属学报, 1988, 24(3): 290-292.
,
.
INFLUENCE OF Al_2O_3 ON DISSOLUTION OF MAGNESITE-CHROME REFRACTORY IN STEEL REFINING SLAG[J]. Acta Metall Sin, 1988, 24(3): 290-292.
1 李柳生,陈肇友.Cr_2O_3含量不同的镁铬耐火材料在炉外精炼渣中的溶蚀,1985,未发表 2 陈肇友,吴学真,叶方保.钢铁,1985;20(11) :33 3 Willshee J C, While J. Trans Br Ceram Soc 1967; 66: 541 |
|