| 金属玻璃(Fe_(55)Ni_(45))_(78)Si_8B_(14)的低温结构弛豫 |
| 蒋方忻;徐炎;杨国斌;李阳;傅秋南 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院;北京钢铁学院 |
|
| LOW TEMPERATURE STRUCTURAL RELAXATION OF METALLIC GLASS (Fe_(55) Ni_(45))_(78)Si_8 B_(14) |
| by JIANG Fangxin; XU Yan; YANG Guobin; LI Yang; FU Qiunan (Beijing: University of Iron and Steel Technology)(Manuscript received 15 July; 1985; revised manuscript 26 March; 1986) |
引用本文:
蒋方忻;徐炎;杨国斌;李阳;傅秋南. 金属玻璃(Fe_(55)Ni_(45))_(78)Si_8B_(14)的低温结构弛豫[J]. 金属学报, 1987, 23(5): 495-497.
,
,
,
,
.
LOW TEMPERATURE STRUCTURAL RELAXATION OF METALLIC GLASS (Fe_(55) Ni_(45))_(78)Si_8 B_(14)[J]. Acta Metall Sin, 1987, 23(5): 495-497.
1 Egami T. Mater Res Bull, 1978; 13: 557 2 Morito N, Egami T. J Non-Cryst Solids, 1984; 61&62: 973 3 Morito N, Egami T. Acta Metall, 1984; 32: 603 4 Scott M G, Kursumovic A. Acta Metall, 1982; 30: 853 5 Van Den Beukel A, Van Der Zwaag S, Mulder A L. Acta Metall, 1984; 32: 1895 6 Bordoni P G. Nuovo Cimento, 1947; 4: 177 7 Nowick A S, Berry B S. Anelastic Relaxation in Crystalline Solids, New York: Academic Press, 1972: 621 8 Weisberg L R, Quimby S L. Phys Rev, 1958; 110: 338 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|