| 低合金高强度焊缝金属组织的研究 |
| 尹士科;王移山;陈佩兰 |
| 冶金工业部钢铁研究总院;冶金工业部钢铁研究总院;冶金工业部钢铁研究总院 |
|
| STRUCTURE OF WELD METAL FOR LOW ALLOY HIGH STRENGTH STEELS |
| by YIN Shike; WANG Yishan; CHEN Peilan (Central Iron and steel Research Institute; Ministry of Metallurgical Industry; Beijing)(Manuscript received 29 May 1986; revised manuscript 17 October 1986) |
引用本文:
尹士科;王移山;陈佩兰. 低合金高强度焊缝金属组织的研究[J]. 金属学报, 1987, 23(5): 498-500.
,
,
.
STRUCTURE OF WELD METAL FOR LOW ALLOY HIGH STRENGTH STEELS[J]. Acta Metall Sin, 1987, 23(5): 498-500.
1 王世亮,尹惠芝,肖闻凌,金属热处理,1982;(8) :1-10 2 井川博,大重広明,田上豊明。溶接学会志,1980;49(7) :467-472 3 井川博,大重広明,田上豊明。溶接学会志,1980;49(8) :533-537 4 康沫狂,管敦惠,郭成道,朱金荣。理化检验(物理),1979;(5) :1-1 5 须藤一,田村今男。金属组织学,东京:丸善出版社,1972 |
|