Please wait a minute...
金属学报  1987, Vol. 23 Issue (4): 349-356    
  论文 本期目录 | 过刊浏览 |
DD3单晶合金的成分设计和实验研究
吴仲棠;温仲元;陈德厚
北京航空材料研究所;北京航空材料研究所;北京航空材料研究所
COMPOSITION DESIGN AND EXPERIMENTAL STUDY OF SINGLE CRYSTAL ALLOY DD3
by WU Zhongtang; WEN Zhongyuan; CHEN Dehou (Institute of Aeronautical Materials; Beijing) (Manuscript received 19 June; 1985; revised manuscript 27 January; 1986)
引用本文:

吴仲棠;温仲元;陈德厚. DD3单晶合金的成分设计和实验研究[J]. 金属学报, 1987, 23(4): 349-356.
, , . COMPOSITION DESIGN AND EXPERIMENTAL STUDY OF SINGLE CRYSTAL ALLOY DD3[J]. Acta Metall Sin, 1987, 23(4): 349-356.

全文: PDF(1192 KB)  
摘要: 本文用渡辺提出的合金设计法进行正交设计计算,并用实验进行验证,最后确定出一种高温性能比较好的单晶合金DD3.其成分可保证具有约60wt-%的γ’相.良好的组织稳定性和优越的综合性能.
Abstract:Orthogonal design calculation of the composition of single crystal has been carried out using the method proposed by Watanabe. The effects of individual elements on the volume fraction of γ' phase, the electron vacancy number and the lattice parameters of γ and γ' phase as well as the lattice misfit between γ matrix and γ' precipitate have been predicted. Based on the calculation, the dependance of composition on microstructure and mechanical properties has been proposed and compared with experimental results. The composition designed by present provides about 60% of volume fraction of γ' in the alloy, good structural tability excellent high temperature mechanical properties were obtained.
收稿日期: 1987-04-18     
1 Erickson J S, Owczarski W A, Curran P M. Met Prog, 1971; 99(3) :58
2 Versnyder F L, Shank M E. Mater Sci Eng, 1970; 6:213
3 Jackson J J, Donachie M J, Henricks R J, Gell M. Met Trans, 1977; 8A:1615
4 Gell M, Duhl D N, Giamei A F. In:Tien J K et al. eds., Proc 4th Int Symp on Superalloys, Metals Park, ASM, 1980:205
5 Strangman T E, Hoppin G S Ⅲ, Phipps C M, Harris K, Schwer R E. In:Tien J K et al. eds., Superalloys, Proc 4th Int Symp on Superalloys, Metals Park, ASM, 1980:215
6 杨洪才.金属学报,1982;18:510
7 青木晃,野田俊治,村田纯教,汤川夏夫,鉄鋼,1982;68:s1346
8 #12
9 渡辺力藏,九重常男,铁鋼,1975;61(9) :2274
10 Decker R F. Strengthening Mechanisms in Nickel Base Superalloys, Symposium: Steel Streng-thing Mechanisms, Zurich, 1969, Greenwich: Climax Molybdenum, 1970:147
11 Woodyatt L R, Sims C T, Beattie H J Jr. Trans AIME, 1966; 236:519
12 原田広史,山崎道夫,铁鋼,1979;(7) :1059-1068
13 Aldred P. S A E 75104