| 镁合金超塑性变形的复合机制 |
| 陈浦泉;赵敏 |
| 哈尔滨工业大学;哈尔滨工业大学 |
|
| A COMPLEX DEFORMATION MECHANISM FOR SUPERPLASTIC DEFORMATION OF Mg ALLOY |
| by CHEN Puquan; ZHAO Min (Harbin Institute of Technology) (Manuscript received 10 May; 1985; revised manuscript 15 February; 1986) |
引用本文:
陈浦泉;赵敏. 镁合金超塑性变形的复合机制[J]. 金属学报, 1987, 23(4): 313-320.
,
.
A COMPLEX DEFORMATION MECHANISM FOR SUPERPLASTIC DEFORMATION OF Mg ALLOY[J]. Acta Metall Sin, 1987, 23(4): 313-320.
1 Ashby M F, Verall R A, Acta Metall, 1973; 21: 149 2 Novikov I I. Acta Metall, 1977; 10: 1139 3 Ball A, Hutchison M M. Met Sci J, 1969; 3: 1 4 Mukherjee A K. Mat Sci Eng, 1971; 8: 83 5 Spingarn J R, Nix W D. Acta Metall, 1979; 27: 171 6 Gifkins R C. Metall Trans. 1976; 17: 1225 7 Gifkins R C. J Mater Sci, 1978: 13: 1926 8 Geckinli A E. Met Sci, 1983; 17: 12 9 杨金风,陈浦泉.宇航学报,1984;1:44 10 陈浦泉,赵敏.金属热处理,1984;(9) :23 11 陈浦泉,赵敏.金属科学与工艺,1985;4(1) :33 12 Chen Puquan(陈浦泉), Zhao Min(赵敏). In: Pro 7th Int Conf on the Strength of Metals and Alloys, New York: Pergamon Press, 1985; 2: 817g |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|