| Cr12Ni2WMoV钢的疲劳条纹与宏观裂纹扩展 |
| 陈传尧;戴蜀娟;高大兴 |
| 华中工学院;华中工学院;华中工学院 |
|
| FATIGUE STRIATION AND MACROCRACK PROPAGATION IN Cr12Ni2WMoV STEEL |
| CHEN Chuanyao; DAI Shujuan; GAO Daxing (Huazhong University of Science and Technology; Wuhan) |
引用本文:
陈传尧;戴蜀娟;高大兴. Cr12Ni2WMoV钢的疲劳条纹与宏观裂纹扩展[J]. 金属学报, 1986, 22(2): 81-86.
,
,
.
FATIGUE STRIATION AND MACROCRACK PROPAGATION IN Cr12Ni2WMoV STEEL[J]. Acta Metall Sin, 1986, 22(2): 81-86.
1 Crooker, T.W. et al., Am. soc. Test. Mater., Spec. Tech. Publ., 600, (1976) , p. 205. 2 Hertzberg, R.W., Deformation and Fracture Mechanics of Engineering Materials, Wiley, New York, 1976, p. 533. 3 陈传尧;高大兴,第二届全国疲劳学术会议论文集(中册);中国力学、航空、机械学会1984,№303. 4 Forman, R.G., et al., Trans. ASME, Ser. D,J. Basic Eng., 89 (1967) , 459. 5 Laird, C., Am. Soc. Test. Mater., Spec. Tech. Publ., 415 (1967) , p. 131 |
|