| 多相材料断裂韧性K_(Ic)的估计 |
| 李中华 |
| 西安交通大学 |
|
| ESTIMATION OF FRACTURE TOUGHNESS FOR POLYCOMPONENT COMPOSITE MATERIALS |
| LI Zhonghua (Xi' an jiaotong University) |
引用本文:
李中华. 多相材料断裂韧性K_(Ic)的估计[J]. 金属学报, 1986, 22(2): 87-92.
.
ESTIMATION OF FRACTURE TOUGHNESS FOR POLYCOMPONENT COMPOSITE MATERIALS[J]. Acta Metall Sin, 1986, 22(2): 87-92.
1 Kameswararao, C.V.S., Eng. Fract. Mech., 18 (1983) , 35. 2 Patton, V.Z.; Morozov, E.M., Elastic Plastic Frature Mechanics, 1978, p. 74. 3 (叶彦谦等译),微积分学教程,第一卷第一分册,p.59. 4 Hagiwara, Y.; Knott, J, F., 5th Int. Conf. on Fracture, Vol. 2, 1981, 707. 5 Kunio, T.; Shimizu, M.; Yamada, K., Fracture Mechanics of Ductile and Tough Materials Applications to Energy Related Sructure, Eds. Liu, H.W.; Kunio, T., Martinus Nijhoff Publ., The Hague/Boston/London, 1980, p. 221. 6 Harris, B.; Cawthorne, D., Plast. and Polym. 42 (1974) , №161, 209. 7 Cawthorne, D.; Harris, B., Composits, 6 (1975) , p. 115. 8 Kaplan, M.F.; ACI J. Proc., 58 (1961) , 591. 9 Swamy, R.N., Fracture Mechanics Applied to Concrete, In Developments in Concrete Tech-nology, Vol. 1, Ed. Lydon, F.D., Applied Science Publ., London, 1978, p. 221. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|