| 高温高速下合金结构钢流动应力研究 |
| 周纪华;管克智 |
| 北京钢铁学院;北京钢铁学院 |
|
| THE FLOW STRESS OF ALLOY STRUCTURAL STEELS AT HIGH TEMPERATURE AND HIGH STRAIN RATE |
| ZHOU Jihua; GUAN Kezhi (Beijing University of Iron and Steel Technology) |
引用本文:
周纪华;管克智. 高温高速下合金结构钢流动应力研究[J]. 金属学报, 1986, 22(1): 123-131.
,
.
THE FLOW STRESS OF ALLOY STRUCTURAL STEELS AT HIGH TEMPERATURE AND HIGH STRAIN RATE[J]. Acta Metall Sin, 1986, 22(1): 123-131.
1 孙一康;孙民生,周纪华,钢铁,14 (1979) .№ 2. 94. 2 #12 3 岡本丰彦,住友金属,12 (1960) ,323. 4 日本鋼鉄協会编,西安重型机械研究所译,轧制理论及其应用,1975,p.125. |
|