NiTi形状记忆合金的应力-应变行为及其显微组织特征
张一;金嘉陵
上海钢铁研究所;上海钢铁研究所
STRESS-STRAIN BEHAVIOUR AND MICROSTRUCTURE OF NiTi SHAPE-MEMORY ALLOY
ZHANG Yi;JIN Jialing Shanghai Institute of Iron and Steel Research
引用本文:

张一;金嘉陵. NiTi形状记忆合金的应力-应变行为及其显微组织特征[J]. 金属学报, 1985, 21(5): 37-142.
, . STRESS-STRAIN BEHAVIOUR AND MICROSTRUCTURE OF NiTi SHAPE-MEMORY ALLOY[J]. Acta Metall Sin, 1985, 21(5): 37-142.

全文: PDF(2935 KB)  
摘要: 本文对51.6at.-%Ni-Ti形状记忆合金在不同热处理状态下的应力-应变曲线和显微组织结构特征,进行了测试和观察.对预马氏体转变现象和可能的机制以及温度诱发马氏体、应变诱发马氏体的形态和亚结构、弥散析出第二相进行了讨论.
Abstract:The stress-strain plot and microstructure of 51.6 at.-% Ni-Ti shape-memory alloywere examined and observed under different heat treatments.The phenomena andpossible machanism o f Premartensitic transition,the morphology and substructureof martensite induced by temperature or strain as well as the dispersed χ-phase pre-cipitation of the alloy were also discussed.
收稿日期: 1985-05-18     
1 金嘉陵,金属学报,20(1984) .
2 金嘉陵等,待发表工作.
3 Aborlfotoh,M.O.;Aboelfotoh,H.A.;Washburn,J.,J.Appl.Phys.,40(1978) ,5230.
4 Wasilewski,R.J.;Butler,S.R.;Hanlon,J.E.,Met.Sci.,J.,1(1967) ,104.
5 Kolomytsev,V.I.;Lobodyuk,V,A.;Khandros,L.G.,Phys.Status Solidi,(a)50(1978) ,127.
6 Kolomytsev;V.I.;Lobodyuk,V.A.;Khandros,L.G.,Phys.Status Solidi,(a)65(1981) ,87.l
No related articles found!