Please wait a minute...
金属学报  1982, Vol. 18 Issue (3): 281-391    
  论文 本期目录 | 过刊浏览 |
Cu-Al-Ni合金马氏体形貌变化与形状记忆效应
谭树松;黄健超;孙孝华;谭雪成
中南矿冶学院;中南矿冶学院;中南矿冶学院;中南矿冶学院
A NOTE ON RELATIONSHIP BETWEEN MARTENSITE MORPHOLOGY AND SHAPE MEMORY EFFECT OF A Cu-Al-Ni ALLOY
Tan Shusong; Huang Jianchao; Sun Xiaohua; Tan Xuecheng (Central-South Institute of Mining and Metallurgy; Changsha)
引用本文:

谭树松;黄健超;孙孝华;谭雪成. Cu-Al-Ni合金马氏体形貌变化与形状记忆效应[J]. 金属学报, 1982, 18(3): 281-391.
, , , . A NOTE ON RELATIONSHIP BETWEEN MARTENSITE MORPHOLOGY AND SHAPE MEMORY EFFECT OF A Cu-Al-Ni ALLOY[J]. Acta Metall Sin, 1982, 18(3): 281-391.

全文: PDF(3598 KB)  
摘要: 用直接观察的方法研究了不同温度和应力情况下,Cu-Al-Ni合金马氏体形貌的变化,并测定试样相应长度的变化。发现“伪弹性”和“形状记忆”效应与马氏体形貌变化密切相关。
Abstract:A direct observation under different temperature and stress is reported of the martensite morphology variation vs the longitudinal change in a Cu-Al-Ni alloy specimen. The results indicate that its pseudo-elasticity and shape memory effect are closely related to the variation of martensite morphology.
收稿日期: 1982-03-18     
1 Krishnan, R. V.; Delaey, L.; Tas, H.; Warlimont, H., J. Mater. Sci., 9 (1974) , 1536.
2 Shimizu, K.; Otsuka, K., Shape Memory Effects, Ed. Perkins J., Planum Press, New York, 1975, p. 59.
No related articles found!