| 玻璃对Pt合金的接触角与其粘度的关系 |
| 宁远涛 |
| 冶金工业部贵金属研究所 |
|
| RELATIONSHIP BETWEEN CONTACT ANGLE FOR GLASS ON Pt ALLOYS AND GLASS VISCOSITY |
| Ning Yuantao (Institute of Precious Metals) |
引用本文:
宁远涛. 玻璃对Pt合金的接触角与其粘度的关系[J]. 金属学报, 1981, 17(6): 695-698.
.
RELATIONSHIP BETWEEN CONTACT ANGLE FOR GLASS ON Pt ALLOYS AND GLASS VISCOSITY[J]. Acta Metall Sin, 1981, 17(6): 695-698.