| Ti-679合金的稳态蠕变 |
| 曹名洲;赵吉祥;苏革;万晓景 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| ON THE STEADY STATE CREEP OF ALLOY Ti-679 |
| Cao Mingzhou; Zhao Jixiang; Su Ge and Wan Xiaojing |
引用本文:
曹名洲;赵吉祥;苏革;万晓景. Ti-679合金的稳态蠕变[J]. 金属学报, 1981, 17(6): 690-694.
,
,
,
.
ON THE STEADY STATE CREEP OF ALLOY Ti-679[J]. Acta Metall Sin, 1981, 17(6): 690-694.
[1] Conarad, H., Demeester, B., Yin, C. and Doner. M., Rate Processes in Plastic Deformation of Materials, Ed. By Li, J. C. M. and Mukheriee, A. K., Cleveland, 1975, p. 175. [2] Surek, T., Kuon, L. G., Luton, M. J. and Jonas, J. J., Rate Processes in Plastic Deformation of Materials, Ed. by J. C. M. Li and A. K. Mukherijee, Cleveland, 1975, p. 629. [3] Paton, N. E. and Mahoney, M. W., Metall. Trans., 7A (1976) , 1685. [4] Conrad, H., Doner, M. and Demesster, B., Titanium Science and Technology, Ed. by R. I. Jaffee, and H. M. Burte, Plenum, New York, 1973, p. 969. [5] Conrad, H. and Jones, R., The Science, Technology and AppLication of Titanium, Ed. by R. I. Jaffee and N. E. Promisel, Pergamon, Oxford, 1970. [6] Winstone, M. R., Rawlings, Rees D. and West, D. R. F., J. Less-Common Met., 39 (1975) , 205. [7] Kohoe, M. and Brromfield, R. W., Titanium Science and Technology, Ed. by R. I. Jaffee and H. M. Butte, Plenum, New York, 1973, p. 2167. [8] Rosen, A. A. and Rotten, A., Mater. Sci. Eng., 22 (1976) , 23.8 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|